Hard particle erosion of silicon carbide and silicon carbide-titanium diboride from room temperature to 1000 C
Hard particle erosion of silicon carbide and silicon carbide-titanium diboride from room temperature to 1000 C
Hard particle erosion of silicon carbide and silicon carbide-titanium diboride from room temperature to 1000 C
Colclough, A. F. (Autor:in) / Yeomans, J. A. (Autor:in)
WEAR -LAUSANNE- ; 209 ; 229-236
01.01.1997
8 pages
Aufsatz (Zeitschrift)
Englisch
DDC:
620.11292
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Preparation method of titanium carbide/titanium diboride composite ceramic particle preform
Europäisches Patentamt | 2021
|Silicon Carbide - Titanium Carbide Nanocomposites: Microstructural Investigation
British Library Online Contents | 1994
|Europäisches Patentamt | 2023
|Oxidation resistance of hafnium diboride—silicon carbide from 1400 to 2000 °C
British Library Online Contents | 2009
|