Preparation of Sr2CeO4 blue phosphor by ultrasonic spray pyrolysis effect of NH4NO3 addition
Preparation of Sr2CeO4 blue phosphor by ultrasonic spray pyrolysis effect of NH4NO3 addition
Preparation of Sr2CeO4 blue phosphor by ultrasonic spray pyrolysis effect of NH4NO3 addition
Kang, M. J. (Autor:in) / Choi, S. Y. (Autor:in)
JOURNAL OF MATERIALS SCIENCE ; 37 ; 2721-2729
01.01.2002
9 pages
Aufsatz (Zeitschrift)
Englisch
DDC:
620.11
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Fine size Sr2CeO4 phosphor particles prepared by spray pyrolysis from polymeric precursor solution
British Library Online Contents | 2006
|Microwave-accelerated hydrothermal synthesis of blue white phosphor: Sr2CeO4
British Library Online Contents | 2004
|YAG:Ce phosphor particles prepared by ultrasonic spray pyrolysis
British Library Online Contents | 2000
|Superfine Sr2CeO4 powder with blue-emission prepared by microemulsion method
British Library Online Contents | 2005
|Synthesis and luminescence of Sr2CeO4 fine particles
British Library Online Contents | 2003
|