Degrading Mechanism on Hydrogen Absorbing-Desorbing Cycle Durability of V- and Ti-Cr-Based BCC-Type Solid Solutions
Degrading Mechanism on Hydrogen Absorbing-Desorbing Cycle Durability of V- and Ti-Cr-Based BCC-Type Solid Solutions
Degrading Mechanism on Hydrogen Absorbing-Desorbing Cycle Durability of V- and Ti-Cr-Based BCC-Type Solid Solutions
Tanaka, H. (Autor:in) / Kuriyama, N. (Autor:in) / Ichikawa, S. (Autor:in) / Senoh, H. (Autor:in) / Naka, N. (Autor:in) / Aihara, K. (Autor:in) / Itoh, H. (Autor:in) / Tsukahara, M. (Autor:in)
MATERIALS SCIENCE FORUM ; 475/479 ; 2481-2484
01.01.2005
4 pages
Aufsatz (Zeitschrift)
Englisch
DDC:
620.11
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
British Library Online Contents | 2006
|Protium Absorbing and Desorbing Characteristics of Mg~2Ni-Mn Alloy
British Library Online Contents | 2000
|British Library Online Contents | 2005
|Wall Stress Induced by Ab-/Desorbing Hydrogen of LaNi~5~-~xAl~x(x=0, 0.3) Hydrogen Storage Bed
British Library Online Contents | 2001
|Low-Cycle Durability of Steels in High-Pressure Hydrogen
British Library Online Contents | 2004
|