Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Plastic deformation behavior of polypropylene/calcium carbonate composites with and without maleic anhydride grafted polypropylene incorporated using the essential work of fracture method
Plastic deformation behavior of polypropylene/calcium carbonate composites with and without maleic anhydride grafted polypropylene incorporated using the essential work of fracture method
Plastic deformation behavior of polypropylene/calcium carbonate composites with and without maleic anhydride grafted polypropylene incorporated using the essential work of fracture method
Gong, G. (Autor:in) / Xie, B. H. (Autor:in) / Yang, W. (Autor:in) / Li, Z. M. (Autor:in) / Lai, S. M. (Autor:in) / Yang, M. B. (Autor:in)
POLYMER TESTING -LONDON- ; 25 ; 98-106
01.01.2006
9 pages
Aufsatz (Zeitschrift)
Englisch
DDC:
620.192
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
British Library Online Contents | 2005
|British Library Online Contents | 2014
|Study on Chlorination of Maleic Anhydride Grafted Polypropylene
British Library Online Contents | 2013
|Preparation and Crystallization of Carbon Nanotube/maleic Anhydride-grafted Polypropylene Composites
British Library Online Contents | 2008
|British Library Online Contents | 2006
|