Toughening of Ti3SiC2 with 3Y-TZP addition by spark plasma sintering
Toughening of Ti3SiC2 with 3Y-TZP addition by spark plasma sintering
Toughening of Ti3SiC2 with 3Y-TZP addition by spark plasma sintering
Shi, S. L. (Autor:in) / Pan, W. (Autor:in)
MATERIALS SCIENCE AND ENGINEERING A ; 447 ; 303-306
01.01.2007
4 pages
Aufsatz (Zeitschrift)
Englisch
DDC:
620.11
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Tribological behavior of Ti3SiC2/(WC-10Co) composites prepared by spark plasma sintering
British Library Online Contents | 2012
|Microstructure and properties of Ti3SiC2/SiC nanocomposites fabricated by spark plasma sintering
British Library Online Contents | 2008
|Fabrication of high-purity ternary carbide Ti3SiC2 by spark plasma sintering technique
British Library Online Contents | 2005
|Synthesis of high-purity Ti3SiC2 and Ti3AlC2 by spark plasma sintering (SPS) technique
British Library Online Contents | 2005
|Fabrication of high-purity Ti3SiC2 by spark plasma sintering (SPS) of elemental powders
British Library Online Contents | 2003
|