Investigation of in-service damage accumulation of Alloy 800HT methanol reformer outlet tubes
Investigation of in-service damage accumulation of Alloy 800HT methanol reformer outlet tubes
Investigation of in-service damage accumulation of Alloy 800HT methanol reformer outlet tubes
Smillie, M.J. (Autor:in) / Olatte, O. (Autor:in) / Thomas, C. (Autor:in) / Levi, T. (Autor:in)
MATERIALS AT HIGH TEMPERATURES ; 24 ; 241-248
01.01.2007
8 pages
Aufsatz (Zeitschrift)
Englisch
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Failure of welded dilution steam coil made of alloy 800HT
British Library Online Contents | 2011
|Behaviour of short cracks in alloy 800HT under biaxial fatigue
British Library Online Contents | 1996
|Corrosion Reason of Outlet Pipe for Preheating Stage in a Methanol Reformer
British Library Online Contents | 2013
|Evolution of the Microstructure in Alloy 800HT under High Temperature Creep Load
British Library Online Contents | 1998
|Carburization performance of Incoloy 800HT in CH4/H2 gas mixtures
British Library Online Contents | 2004
|