Wavy Imperfections and the Strength of Cast-in-Place Pressure Pipe Liners
The installation of resin-impregnated felt tubes within cast iron water pipes can lead to wavy imperfections (wrinkles) if the external circumference of the liner exceeds the internal circumference of the cast iron pipe. A split-disk test apparatus has been developed and a series of laboratory experiments have been conducted to measure the strength of liners with wavy imperfections. The design of the test apparatus is described, and results are reported for liners installed within cast iron pipes of six inch nominal internal diameter. Results for three different kinds of imperfections are provided, where measurements of maximum hoop force are related to the imperfection size (wavelength and amplitude). Most tests resulted in failures at or in the vicinity of the wrinkles. As the wrinkle size increased, the ultimate strength of the liner and its strength at first cracking were reduced. However, the effect was more detrimental on the latter than the former.
Wavy Imperfections and the Strength of Cast-in-Place Pressure Pipe Liners
The installation of resin-impregnated felt tubes within cast iron water pipes can lead to wavy imperfections (wrinkles) if the external circumference of the liner exceeds the internal circumference of the cast iron pipe. A split-disk test apparatus has been developed and a series of laboratory experiments have been conducted to measure the strength of liners with wavy imperfections. The design of the test apparatus is described, and results are reported for liners installed within cast iron pipes of six inch nominal internal diameter. Results for three different kinds of imperfections are provided, where measurements of maximum hoop force are related to the imperfection size (wavelength and amplitude). Most tests resulted in failures at or in the vicinity of the wrinkles. As the wrinkle size increased, the ultimate strength of the liner and its strength at first cracking were reduced. However, the effect was more detrimental on the latter than the former.
Wavy Imperfections and the Strength of Cast-in-Place Pressure Pipe Liners
Ampiah, Nancy (Autor:in) / Fam, Amir (Autor:in) / Moore, Ian D. (Autor:in)
International Pipelines Conference 2008 ; 2008 ; Atlanta, Georgia, United States
Pipelines 2008 ; 1-10
17.07.2008
Aufsatz (Konferenz)
Elektronische Ressource
Englisch
British Library Online Contents | 2010
|Installed Geometry of Cast-in-Place Polymer Sewer Liners
Online Contents | 2007
|Modelling of cast-in-place concrete tunnel liners condition
Taylor & Francis Verlag | 2020
|