Assessing the autogenous shrinkage cracking propensity of concrete by means of the restrained ring test
The autogenous shrinkage due to self-desiccation of high- and ultra-high performance concretes with very low water-cement ratio in case of restraint leads to considerable stresses starting from very early age. The resultant risk of cracking presently cannot be adequately investigated. Parameters that are particularly difficult to capture experimentally are the concrete temperature and the viscoelasticity. The primary objective of this work was to assess as precise as possible the autogenous shrinkage cracking propensity of representative concretes at strong restraint and constant room temperature. Test methods needed to be chosen and enhanced in a way that preferably allowed for the efficient and precise investigation of all relevant factors in the future. Ideally, a method suitable for a complete empirical modeling was provided. First the methodological requirements and the advantages and disadvantages of existing test methods were discussed. Based on this, optimized test methods were proposed. Their suitability was verified using the example of ultra-high strength concrete. The choice of concrete compositions considered the essential measures for reducing shrinkage (internal curing, shrinkage-reducing admixtures, reduction of the fraction of Portland cement in the binder). The autogenous shrinkage was measured with the shrinkage cone method. This new test method was validated by investigations of the repeatability and reproducibility and proved efficient and precise. It allows for measurements under non-isothermal conditions; no established test method exists for that purpose to date. The autogenous shrinkage of the ultra-high strength concretes at the age of 24 h, investigated under quasi-isothermal conditions (20 °C), was between 0,25 mm/m and 0,70 mm/m. It was particularly low when a shrinkage-reducing admixture was added and when superabsorbent polymers were used. The stresses due to restraint were determined with the restrained ring test. A large part of the stresses to be expected according to Hooke’s ...
Assessing the autogenous shrinkage cracking propensity of concrete by means of the restrained ring test
The autogenous shrinkage due to self-desiccation of high- and ultra-high performance concretes with very low water-cement ratio in case of restraint leads to considerable stresses starting from very early age. The resultant risk of cracking presently cannot be adequately investigated. Parameters that are particularly difficult to capture experimentally are the concrete temperature and the viscoelasticity. The primary objective of this work was to assess as precise as possible the autogenous shrinkage cracking propensity of representative concretes at strong restraint and constant room temperature. Test methods needed to be chosen and enhanced in a way that preferably allowed for the efficient and precise investigation of all relevant factors in the future. Ideally, a method suitable for a complete empirical modeling was provided. First the methodological requirements and the advantages and disadvantages of existing test methods were discussed. Based on this, optimized test methods were proposed. Their suitability was verified using the example of ultra-high strength concrete. The choice of concrete compositions considered the essential measures for reducing shrinkage (internal curing, shrinkage-reducing admixtures, reduction of the fraction of Portland cement in the binder). The autogenous shrinkage was measured with the shrinkage cone method. This new test method was validated by investigations of the repeatability and reproducibility and proved efficient and precise. It allows for measurements under non-isothermal conditions; no established test method exists for that purpose to date. The autogenous shrinkage of the ultra-high strength concretes at the age of 24 h, investigated under quasi-isothermal conditions (20 °C), was between 0,25 mm/m and 0,70 mm/m. It was particularly low when a shrinkage-reducing admixture was added and when superabsorbent polymers were used. The stresses due to restraint were determined with the restrained ring test. A large part of the stresses to be expected according to Hooke’s ...
Assessing the autogenous shrinkage cracking propensity of concrete by means of the restrained ring test
14.03.2011
Hochschulschrift
Elektronische Ressource
Englisch
info:eu-repo/classification/ddc/690 , ddc:690 , Ultrahochfester Beton , Autogenes Schwinden , Rissneigung , Zwang , Ring-Test , Spaltzugfestigkeit , Schwindkegelverfahren , Kriechen , Relaxation , Temperatur , sehr frühes Alter , Ultra-high-strength concrete , autogenous shrinkage , cracking propensity , restrained ring test , splitting tensile strength , shrinkage cone method , creep , temperature , very early age
TIBKAT | 2011
|UB Braunschweig | 2011
|Detection of early-age cracking due to restrained autogenous shrinkage
British Library Conference Proceedings | 2007
|