Internal friction peak near 220 K of work-hardened zirconium-copper alloys
Damping of vibration of order of 13 kc show maximum near temperature of 220 K; characteristics of peak are in general agreement with Bordoni theory.
Internal friction peak near 220 K of work-hardened zirconium-copper alloys
Damping of vibration of order of 13 kc show maximum near temperature of 220 K; characteristics of peak are in general agreement with Bordoni theory.
Internal friction peak near 220 K of work-hardened zirconium-copper alloys
Pic de frottement interieur au voisinage de 220° K dans les alliages zirconium-cuivre ecrouis
Boch, P. (Autor:in) / Petit, J. (Autor:in) / Gasc, C. (Autor:in) / de Fouquet, J. (Autor:in)
1968
3 pages
Aufsatz (Zeitschrift)
Französisch
© Metadata Copyright Elsevier B. V. All rights reserved.
A new low-temperature internal friction peak in NiTi based alloys
British Library Online Contents | 2006
|Hydrogen Internal Friction Peak in Amorphous Zr-Cu-Al-Si Alloys
British Library Online Contents | 2002
|Friction Stir Welding of Precipitation Hardened Ni Based Alloys
British Library Online Contents | 2007
|Electron microscopic pictures of hardened aluminum copper alloys
Engineering Index Backfile | 1949
|Electron microscopic pictures of hardened aluminum copper alloys
Engineering Index Backfile | 1949
|