Sintering of polycrystalline diamond cutting tools
AbstractIn this study, pressure-sintering experiments during direct sintering of diamond cutting tools has been conducted at 730°C for 3–15min with a pressure of around 350MPa. For the matrix, the elements cobalt and nickel are used as the bonding phase and the α-bronze is used as the filling phase in various amounts. In microstructural characterization studies, various microstructural analyses were performed using the techniques of light microscopy, scanning electron microscopy (SEM), energy-disperse X-ray spectrography and image analysis.
Sintering of polycrystalline diamond cutting tools
AbstractIn this study, pressure-sintering experiments during direct sintering of diamond cutting tools has been conducted at 730°C for 3–15min with a pressure of around 350MPa. For the matrix, the elements cobalt and nickel are used as the bonding phase and the α-bronze is used as the filling phase in various amounts. In microstructural characterization studies, various microstructural analyses were performed using the techniques of light microscopy, scanning electron microscopy (SEM), energy-disperse X-ray spectrography and image analysis.
Sintering of polycrystalline diamond cutting tools
Zeren, Muzaffer (Autor:in) / Karagöz, Şadi (Autor:in)
26.09.2005
4 pages
Aufsatz (Zeitschrift)
Elektronische Ressource
Englisch
Sintering of polycrystalline diamond cutting tools
British Library Online Contents | 2007
|Europäisches Patentamt | 2015
|Europäisches Patentamt | 2018
|Europäisches Patentamt | 2016
|Europäisches Patentamt | 2016
|