DELAYED, SWELLABLE PARTICLES FOR PREVENTION OF FLUID MIGRATION THROUGH DAMAGED CEMENT SHEATHS
A method includes providing a cementing composition that includes an aqueous fluid, a cementitious particulate, and a copolymer particulate which includes a monofunctional monomer, a water degradable first crosslinker, and a second crosslinker. The method further includes placing the cementing composition in a subterranean formation so as to form a set cement sheath and swelling the copolymer particulate in response to a void created in the set cement sheath. The copolymer particulate allows the cementing composition to set to form the cement sheath before substantial swelling of the copolymer particulate occurs.
Cette invention concerne un procédé de préparation d'une composition de cimentation qui comprend un fluide aqueux, un matériau particulaire à base de ciment, et un matériau particulaire copolymère qui contient un monomère monofonctionnel, un premier agent de réticulation hydrodégradable, et un second agent de réticulation. Le procédé selon l'invention concerne en outre le placement de la composition de cimentation dans une formation souterraine de façon à former une gaine de ciment destiné à prendre et le gonflement du matériau particulaire copolymère en réponse à un vide créé dans la gaine une fois le ciment pris. Le matériau particulaire copolymère permet à la composition de cimentation de prendre pour former la gaine de ciment avant que le gonflement sensible du matériau particulaire copolymère ne se produise.
DELAYED, SWELLABLE PARTICLES FOR PREVENTION OF FLUID MIGRATION THROUGH DAMAGED CEMENT SHEATHS
A method includes providing a cementing composition that includes an aqueous fluid, a cementitious particulate, and a copolymer particulate which includes a monofunctional monomer, a water degradable first crosslinker, and a second crosslinker. The method further includes placing the cementing composition in a subterranean formation so as to form a set cement sheath and swelling the copolymer particulate in response to a void created in the set cement sheath. The copolymer particulate allows the cementing composition to set to form the cement sheath before substantial swelling of the copolymer particulate occurs.
Cette invention concerne un procédé de préparation d'une composition de cimentation qui comprend un fluide aqueux, un matériau particulaire à base de ciment, et un matériau particulaire copolymère qui contient un monomère monofonctionnel, un premier agent de réticulation hydrodégradable, et un second agent de réticulation. Le procédé selon l'invention concerne en outre le placement de la composition de cimentation dans une formation souterraine de façon à former une gaine de ciment destiné à prendre et le gonflement du matériau particulaire copolymère en réponse à un vide créé dans la gaine une fois le ciment pris. Le matériau particulaire copolymère permet à la composition de cimentation de prendre pour former la gaine de ciment avant que le gonflement sensible du matériau particulaire copolymère ne se produise.
DELAYED, SWELLABLE PARTICLES FOR PREVENTION OF FLUID MIGRATION THROUGH DAMAGED CEMENT SHEATHS
PARTICULES A EFFET RETARD, APTES AU GONFLEMENT POUR PREVENIR LA MIGRATION DES FLUIDES A TRAVERS DES GAINES DE CIMENT ENDOMMAGEES
FUNKHOUSER GARY P (Autor:in) / BENKLEY JAMES R (Autor:in)
25.07.2017
Patent
Elektronische Ressource
Englisch
FOAMED CEMENT COMPOSITIONS COMPRISING OIL-SWELLABLE PARTICLES AND METHODS OF USE
Europäisches Patentamt | 2015
|Swellable glass particles for reducing fluid flow in subterranean formations
Europäisches Patentamt | 2018
|