The invention discloses a corrosion-resistant concrete which is prepared from the following raw materials, by weight: 0.4-0.9 parts of a TG cementing agent, 0.2-0.4 parts of coke, 3.5-4.5 parts of molasses, 0.1-0.3 parts of sodium carbonate, 0.2-0.4 parts of sodium thiosulfate, 5-12 parts of hollow glass microspheres, 0.8-1 part of sodium nitrate, 1-5 parts of a naphthalene-series water-reducing agent, 1-3 parts of stearic acid, 0.1-0.3 parts of glass fiber, 0.2-0.4 parts of tetrahydroxyethyl ethylenediamine, 5-10 parts of diatomite, 1-3 parts of modified coated clay, 1-3 parts of re-burned magnesium oxide, 0.2-0.5 parts of magnesium stearate, 10-15 parts of dolomite, 30-40 parts of white cement, and 2-3 parts of oxidized starch.
The invention discloses a corrosion-resistant concrete which is prepared from the following raw materials, by weight: 0.4-0.9 parts of a TG cementing agent, 0.2-0.4 parts of coke, 3.5-4.5 parts of molasses, 0.1-0.3 parts of sodium carbonate, 0.2-0.4 parts of sodium thiosulfate, 5-12 parts of hollow glass microspheres, 0.8-1 part of sodium nitrate, 1-5 parts of a naphthalene-series water-reducing agent, 1-3 parts of stearic acid, 0.1-0.3 parts of glass fiber, 0.2-0.4 parts of tetrahydroxyethyl ethylenediamine, 5-10 parts of diatomite, 1-3 parts of modified coated clay, 1-3 parts of re-burned magnesium oxide, 0.2-0.5 parts of magnesium stearate, 10-15 parts of dolomite, 30-40 parts of white cement, and 2-3 parts of oxidized starch.
Corrosion-resistant concrete
WANG XIAOBO (Autor:in)
22.04.2015
Patent
Elektronische Ressource
Englisch
IPC:
C04B
Kalk
,
LIME