Porous material with central symmetry structure and method for preparing the same
The invention discloses a porous material with a central symmetry structure. Layered holes of the porous material are of a central symmetry oriented structure along the radial cross section. A method for preparing the porous material with the central symmetry structure comprises adding a dispersing agent and adhesives in water, adding ceramic powder after uniform mixing, using a zirconia ball or an alumina ball as a ball milling medium to perform ball milling, obtaining slurry with the volume concentration of 20%-40%; injecting the slurry in a cylindrical die with the side face and the bottom surface provided with a heat transfer material, placing the die on a freezing partition plate of a freezing dryer to freeze the slurry for 2-4 h, causing the freezing temperature to be -50 DEG C to -30 DEG C; completely freezing the slurry and then taking the slurry out of the die, placing the frozen slurry in the environment with the pressure of 0-600 Pa to perform low pressure drying for 20-24 h, so as to obtain a porous material prefabricated body; and finally sintering the porous material prefabricated body in the air or in the atmosphere of vacuum at 800-1700 DEG C for 2-3 h to obtain the porous material.
Porous material with central symmetry structure and method for preparing the same
The invention discloses a porous material with a central symmetry structure. Layered holes of the porous material are of a central symmetry oriented structure along the radial cross section. A method for preparing the porous material with the central symmetry structure comprises adding a dispersing agent and adhesives in water, adding ceramic powder after uniform mixing, using a zirconia ball or an alumina ball as a ball milling medium to perform ball milling, obtaining slurry with the volume concentration of 20%-40%; injecting the slurry in a cylindrical die with the side face and the bottom surface provided with a heat transfer material, placing the die on a freezing partition plate of a freezing dryer to freeze the slurry for 2-4 h, causing the freezing temperature to be -50 DEG C to -30 DEG C; completely freezing the slurry and then taking the slurry out of the die, placing the frozen slurry in the environment with the pressure of 0-600 Pa to perform low pressure drying for 20-24 h, so as to obtain a porous material prefabricated body; and finally sintering the porous material prefabricated body in the air or in the atmosphere of vacuum at 800-1700 DEG C for 2-3 h to obtain the porous material.
Porous material with central symmetry structure and method for preparing the same
TANG YUFEI (Autor:in) / QIU SHA (Autor:in) / ZHAO KANG (Autor:in) / WU CONG (Autor:in)
30.09.2015
Patent
Elektronische Ressource
Englisch
Method for preparing porous carbon material and porous carbon material obtainable by same
Europäisches Patentamt | 2021
|