Nano-grade modified sintered brick and production method thereof
The invention discloses a nano-grade modified sintered brick and a production method thereof. The brick is prepared from the raw materials of, by weight, 2-4 parts of nano-grade alumina, 10-15 parts of sculpture clay, 8-12 parts of sea mud, 5-10 parts of polyvinyl acetate, 4-6 parts of tung oil, 3-6 parts of waste syrup, 1-2 parts of sodium lauroyl sarcosinate, 3-5 parts of fir balsam, 4-8 parts of asbestos fiber, 6-8 parts of an additive, a proper amount of water, and the like. According to the invention, waste brick slag is adopted as a main raw material, such that clay resource is saved, production cost is reduced, a waste brick slag treatment problem is solved, and environment pollution caused by the waste brick slag is avoided. The sintered brick provided by the invention has the advantages of high strength, high bearing capacity, low density, low heat conductivity coefficient, wide application range, and good market prospect. The sintered brick meets the requirements of users. The added polyurethane elastomer has excellent wear resistance and oil resistance, and is a polar polymer which can be organically combined with polypropylene, such that polypropylene mechanical performances can be improved. The added fluororubber has the characteristics of high-temperature resistance, oil resistance and the like. With the other fillers other physical performances and processing performances can be enhanced.
Nano-grade modified sintered brick and production method thereof
The invention discloses a nano-grade modified sintered brick and a production method thereof. The brick is prepared from the raw materials of, by weight, 2-4 parts of nano-grade alumina, 10-15 parts of sculpture clay, 8-12 parts of sea mud, 5-10 parts of polyvinyl acetate, 4-6 parts of tung oil, 3-6 parts of waste syrup, 1-2 parts of sodium lauroyl sarcosinate, 3-5 parts of fir balsam, 4-8 parts of asbestos fiber, 6-8 parts of an additive, a proper amount of water, and the like. According to the invention, waste brick slag is adopted as a main raw material, such that clay resource is saved, production cost is reduced, a waste brick slag treatment problem is solved, and environment pollution caused by the waste brick slag is avoided. The sintered brick provided by the invention has the advantages of high strength, high bearing capacity, low density, low heat conductivity coefficient, wide application range, and good market prospect. The sintered brick meets the requirements of users. The added polyurethane elastomer has excellent wear resistance and oil resistance, and is a polar polymer which can be organically combined with polypropylene, such that polypropylene mechanical performances can be improved. The added fluororubber has the characteristics of high-temperature resistance, oil resistance and the like. With the other fillers other physical performances and processing performances can be enhanced.
Nano-grade modified sintered brick and production method thereof
SHANGGUAN TING (Autor:in)
28.10.2015
Patent
Elektronische Ressource
Englisch
Coal gangue sintered brick and production method thereof
Europäisches Patentamt | 2015
|Yellow sintered landscape brick and production method thereof
Europäisches Patentamt | 2015
|Sintered brick production equipment and production process thereof
Europäisches Patentamt | 2022
|Red sintered shale landscape brick and production method thereof
Europäisches Patentamt | 2015
|Subway shield muck sintered brick and production method thereof
Europäisches Patentamt | 2023
|