Environment-friendly bamboo charcoal sintered brick
The invention discloses an environment-friendly bamboo charcoal sintered brick. The environment-friendly bamboo charcoal sintered brick is prepared from, by weight, 1-2 parts of compound coagulant, 0.2-0.4 part of calcium lignosulphonate, 0.1-0.2 part of calcium nitrate, 1-3 parts of soda dregs, 13-15 parts of talcum powder, 10-17 parts of zeolite powder, 1-3 parts of bamboo carbon powder, 1-2 parts of lauryl sodium sulfate, 0.3-0.5 part of stearic acid, 0.1-0.2 part of calcium sorbate, 20-30 parts of shale-fly, 20-30 parts of clay, 10-20 parts of syderolite, 0.1-0.3 part of carboxylic butadiene-styrene latex, 10-20 parts of opal powder and 0.2-0.4 part of calcium stearate. The soda dregs mainly include waste residues using calcium salt such as calcium carbonate, calcium sulfate and calcium chloride as the main components, and further include the components such as a small amount of sulfur dioxide; when the soda dregs are used for preparing the sintered brick, the strength of the sintered brick can be improved, and meanwhile waste can be turned into wealth. Bamboo charcoal is added, so that environmental protection can be achieved, and the bamboo charcoal can load hazardous substances through pores together with the zeolite powder.
Environment-friendly bamboo charcoal sintered brick
The invention discloses an environment-friendly bamboo charcoal sintered brick. The environment-friendly bamboo charcoal sintered brick is prepared from, by weight, 1-2 parts of compound coagulant, 0.2-0.4 part of calcium lignosulphonate, 0.1-0.2 part of calcium nitrate, 1-3 parts of soda dregs, 13-15 parts of talcum powder, 10-17 parts of zeolite powder, 1-3 parts of bamboo carbon powder, 1-2 parts of lauryl sodium sulfate, 0.3-0.5 part of stearic acid, 0.1-0.2 part of calcium sorbate, 20-30 parts of shale-fly, 20-30 parts of clay, 10-20 parts of syderolite, 0.1-0.3 part of carboxylic butadiene-styrene latex, 10-20 parts of opal powder and 0.2-0.4 part of calcium stearate. The soda dregs mainly include waste residues using calcium salt such as calcium carbonate, calcium sulfate and calcium chloride as the main components, and further include the components such as a small amount of sulfur dioxide; when the soda dregs are used for preparing the sintered brick, the strength of the sintered brick can be improved, and meanwhile waste can be turned into wealth. Bamboo charcoal is added, so that environmental protection can be achieved, and the bamboo charcoal can load hazardous substances through pores together with the zeolite powder.
Environment-friendly bamboo charcoal sintered brick
CHEN RONGFA (Autor:in)
25.11.2015
Patent
Elektronische Ressource
Englisch
IPC:
C04B
Kalk
,
LIME
Environment-friendly wall structure based on bamboo charcoal anion coating
Europäisches Patentamt | 2023
|Bamboo charcoal powder-containing low energy consumption aerated brick
Europäisches Patentamt | 2015
|Method for preparing environment-friendly baking-free brick from biomass charcoal
Europäisches Patentamt | 2022
|Rectangular hole light shale sintered environment-friendly perforated brick