Polyphenyl granule mortar additive, polyphenyl granule mortar and preparation method of polyphenyl granule mortar
The invention provides a polyphenyl granule mortar additive, polyphenyl granule mortar and a preparation method of the polyphenyl granule mortar. The polyphenyl granule mortar additive comprises 15-30parts of a modifier, 5-10 parts of a water reducing agent, 5-10 parts of cellulose, 5-15 parts of latex powder, 0.5-1.5 parts of an air entraining agent, 2-8 parts of plant fibers, 1-3 parts of a foam stabilizer, 30-40 parts of an early strength agent, 1-5 parts of an excitant and 1-5 parts of C9 resin. The polyphenyl granule mortar comprises 500 to 1000 parts of cement, 100 to 700 parts of coalash, 10 to 50 parts of polyphenyl granules, 500 to 750 parts of water and 80 to 100 parts of polyphenyl granule mortar additive. The preparation method comprises the steps: uniformly mixing the raw materials, adding water, and stirring to obtain the polyphenyl granule mortar. According to the polyphenyl granule mortar additive and the mortar provided by the invention, mold expansion caused by hydration heat can be reduced, the slurry bonding force is improved, the strength effect is enhanced, the early strength is improved, and the mold removal time is shortened.
本发明提供一种聚苯颗粒砂浆添加剂、聚苯颗粒砂浆及其制备方法。聚苯颗粒砂浆添加剂包括:改性剂15‑30份、减水剂5‑10份、纤维素5‑10份、乳胶粉5‑15份、引气剂0.5‑1.5份、植物纤维2‑8份、稳泡剂1‑3份、早强剂30‑40份、激发剂1‑5份和C9树脂1‑5份。聚苯颗粒砂浆包括:水泥500‑1000份、粉煤灰100‑700份、聚苯颗粒10‑50份、水500‑750份以及聚苯颗粒砂浆添加剂80‑100份。制备方法:将各原料混合均匀,加入水搅拌得到聚苯颗粒砂浆。本申请提供的聚苯颗粒砂浆添加剂和砂浆,能够降低因水化热涨模,提高浆体粘接力,增加强度效应,提高早期强度,缩短拆模时间。
Polyphenyl granule mortar additive, polyphenyl granule mortar and preparation method of polyphenyl granule mortar
The invention provides a polyphenyl granule mortar additive, polyphenyl granule mortar and a preparation method of the polyphenyl granule mortar. The polyphenyl granule mortar additive comprises 15-30parts of a modifier, 5-10 parts of a water reducing agent, 5-10 parts of cellulose, 5-15 parts of latex powder, 0.5-1.5 parts of an air entraining agent, 2-8 parts of plant fibers, 1-3 parts of a foam stabilizer, 30-40 parts of an early strength agent, 1-5 parts of an excitant and 1-5 parts of C9 resin. The polyphenyl granule mortar comprises 500 to 1000 parts of cement, 100 to 700 parts of coalash, 10 to 50 parts of polyphenyl granules, 500 to 750 parts of water and 80 to 100 parts of polyphenyl granule mortar additive. The preparation method comprises the steps: uniformly mixing the raw materials, adding water, and stirring to obtain the polyphenyl granule mortar. According to the polyphenyl granule mortar additive and the mortar provided by the invention, mold expansion caused by hydration heat can be reduced, the slurry bonding force is improved, the strength effect is enhanced, the early strength is improved, and the mold removal time is shortened.
本发明提供一种聚苯颗粒砂浆添加剂、聚苯颗粒砂浆及其制备方法。聚苯颗粒砂浆添加剂包括:改性剂15‑30份、减水剂5‑10份、纤维素5‑10份、乳胶粉5‑15份、引气剂0.5‑1.5份、植物纤维2‑8份、稳泡剂1‑3份、早强剂30‑40份、激发剂1‑5份和C9树脂1‑5份。聚苯颗粒砂浆包括:水泥500‑1000份、粉煤灰100‑700份、聚苯颗粒10‑50份、水500‑750份以及聚苯颗粒砂浆添加剂80‑100份。制备方法:将各原料混合均匀,加入水搅拌得到聚苯颗粒砂浆。本申请提供的聚苯颗粒砂浆添加剂和砂浆,能够降低因水化热涨模,提高浆体粘接力,增加强度效应,提高早期强度,缩短拆模时间。
Polyphenyl granule mortar additive, polyphenyl granule mortar and preparation method of polyphenyl granule mortar
聚苯颗粒砂浆添加剂、聚苯颗粒砂浆及其制备方法
YANG BIN (Autor:in) / WANG JINHU (Autor:in) / YU XIAOLEI (Autor:in) / GONG CHANGFENG (Autor:in) / LI YANHUA (Autor:in)
29.05.2020
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Preparation method of rubber powder polyphenyl granule thermal insulation mortar
Europäisches Patentamt | 2020
|Dry-mixed polyphenyl granule thermal insulation mortar and preparation method thereof
Europäisches Patentamt | 2015
|Europäisches Patentamt | 2020
|