Clay sculpture material and preparation method thereof
The invention relates to a clay carving material prepared from the following components in parts by weight: 20-30 parts of calcium carbonate, 15-20 parts of liquid paraffin, 8-12 parts of glycerol, 40-60 parts of mud main materials, 3-6 parts of vitamin gum, 3-5 parts of semi-hydrated gypsum and 8-12 parts of vinyl tri(dimethylsiloxane) silane/isocyano ethyl methacrylate/rosin modified chlorogenicacid copolymer. The invention further discloses a preparation method of the clay sculpture material. The clay sculpture material is better in comprehensive performance, water resistance and mechanical property, more excellent in performance stability and longer in plasticity retention time, and sculptured clay sculptures are firm, attractive and durable; according to the method, a complex processthat the clay sculpture material needs to be fired in the cave at high temperature is overcome, the effect of hardening and forming the clay can be achieved through a common flame spray gun, and higheconomic value and social value are achieved.
本发明涉及一种泥雕刻材料,其包括如下重量份的各组分制成:碳酸钙20‑30份、液体石蜡15‑20份、甘油8‑12份、泥主料40‑60份、维生素胶3‑6份、半水石膏3‑5份、乙烯基三(二甲基硅氧烷基)硅烷/甲基丙烯酸异氰基乙酯/松香改性绿原酸共聚物8‑12份。本发明还公开了所述泥雕刻材料的制备方法。本发明公开的泥雕刻材料综合性能更佳,耐水性和机械力学性能更好,性能稳定性更优异,可塑性保持时间更长,雕塑出来的泥雕结实、美观、耐用;克服了泥雕材料需要到窑洞中高温烧制的繁琐流程,通过普通火焰喷枪,就可以达到泥土硬化成型的效果,具有较高的经济价值和社会价值。
Clay sculpture material and preparation method thereof
The invention relates to a clay carving material prepared from the following components in parts by weight: 20-30 parts of calcium carbonate, 15-20 parts of liquid paraffin, 8-12 parts of glycerol, 40-60 parts of mud main materials, 3-6 parts of vitamin gum, 3-5 parts of semi-hydrated gypsum and 8-12 parts of vinyl tri(dimethylsiloxane) silane/isocyano ethyl methacrylate/rosin modified chlorogenicacid copolymer. The invention further discloses a preparation method of the clay sculpture material. The clay sculpture material is better in comprehensive performance, water resistance and mechanical property, more excellent in performance stability and longer in plasticity retention time, and sculptured clay sculptures are firm, attractive and durable; according to the method, a complex processthat the clay sculpture material needs to be fired in the cave at high temperature is overcome, the effect of hardening and forming the clay can be achieved through a common flame spray gun, and higheconomic value and social value are achieved.
本发明涉及一种泥雕刻材料,其包括如下重量份的各组分制成:碳酸钙20‑30份、液体石蜡15‑20份、甘油8‑12份、泥主料40‑60份、维生素胶3‑6份、半水石膏3‑5份、乙烯基三(二甲基硅氧烷基)硅烷/甲基丙烯酸异氰基乙酯/松香改性绿原酸共聚物8‑12份。本发明还公开了所述泥雕刻材料的制备方法。本发明公开的泥雕刻材料综合性能更佳,耐水性和机械力学性能更好,性能稳定性更优异,可塑性保持时间更长,雕塑出来的泥雕结实、美观、耐用;克服了泥雕材料需要到窑洞中高温烧制的繁琐流程,通过普通火焰喷枪,就可以达到泥土硬化成型的效果,具有较高的经济价值和社会价值。
Clay sculpture material and preparation method thereof
一种泥雕刻材料及其制备方法
CHEN HONGXIN (Autor:in) / JIANG WEI (Autor:in) / TANG HUI (Autor:in) / ZHANG ZHEN (Autor:in) / ZHOU CHUNWANG (Autor:in) / ZHANG LIN (Autor:in) / CHANG YINGJUN (Autor:in) / QIAN LONGJUN (Autor:in)
12.06.2020
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Novel environment-friendly clay sculpture material and manufacturing method thereof
Europäisches Patentamt | 2020
|Improved clay painted sculpture material process method
Europäisches Patentamt | 2022
|Sculpture cement material and preparation method thereof
Europäisches Patentamt | 2021
|Europäisches Patentamt | 2024
|