Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Metal dry granular glaze, matte metallic luster ceramic tile and preparation method of matte metallic luster ceramic tile
The invention discloses a metal dry granular glaze, a matte metallic luster ceramic tile and a preparation method of the matte metallic luster ceramic tile. The metal dry granular glaze is prepared from the following components: SiO2, Al2O3, CaO, MgO, K2O, Na2O, B2O3, Cr2O3, NiO, CoO, Fe2O3, CuO, SnO2 and MnO; through synergistic optimization of the basic glaze and other components, the glaze canbe good in stability and corrosion resistance without using a metal element containing lead which is harmful to a human body and the environment, the polished ceramic tile surface has strong silver bright metal luster under illumination, the hardness reaches grade 6, and the wear resistance is 2100 revolutions or above. The preparation method of the ceramic tile is simple, one-time firing is achieved, simultaneous maturation of the green brick, the cover glaze layer and the metal dry granular glaze layer is facilitated, formation of the middle layer is facilitated, and the rigidity of the ceramic tile is improved.
本发明公开了一种金属干粒釉料、哑光金属光泽瓷砖及其制备方法;所述的金属干粒釉料包括如下组分:SiO2、Al2O3、CaO、MgO、K2O、Na2O、B2O3、Cr2O3、NiO、CoO、Fe2O3、CuO、SnO2和MnO;通过对基础釉料以及其它组分的协同优化,无需使用含铅这一种对人体、环境有危害的金属元素即可使釉料的稳定性好,耐腐蚀性能佳,抛光后的瓷砖砖面在光照下具有强烈的银亮色金属光泽,而且硬度达到6级、耐磨2100转以上;所述瓷砖的制备方法简单,一次烧成,有利于砖坯、面釉层、金属干粒釉层的同时成熟,有利于中间层的形成,提高瓷砖的刚性。
Metal dry granular glaze, matte metallic luster ceramic tile and preparation method of matte metallic luster ceramic tile
The invention discloses a metal dry granular glaze, a matte metallic luster ceramic tile and a preparation method of the matte metallic luster ceramic tile. The metal dry granular glaze is prepared from the following components: SiO2, Al2O3, CaO, MgO, K2O, Na2O, B2O3, Cr2O3, NiO, CoO, Fe2O3, CuO, SnO2 and MnO; through synergistic optimization of the basic glaze and other components, the glaze canbe good in stability and corrosion resistance without using a metal element containing lead which is harmful to a human body and the environment, the polished ceramic tile surface has strong silver bright metal luster under illumination, the hardness reaches grade 6, and the wear resistance is 2100 revolutions or above. The preparation method of the ceramic tile is simple, one-time firing is achieved, simultaneous maturation of the green brick, the cover glaze layer and the metal dry granular glaze layer is facilitated, formation of the middle layer is facilitated, and the rigidity of the ceramic tile is improved.
本发明公开了一种金属干粒釉料、哑光金属光泽瓷砖及其制备方法;所述的金属干粒釉料包括如下组分:SiO2、Al2O3、CaO、MgO、K2O、Na2O、B2O3、Cr2O3、NiO、CoO、Fe2O3、CuO、SnO2和MnO;通过对基础釉料以及其它组分的协同优化,无需使用含铅这一种对人体、环境有危害的金属元素即可使釉料的稳定性好,耐腐蚀性能佳,抛光后的瓷砖砖面在光照下具有强烈的银亮色金属光泽,而且硬度达到6级、耐磨2100转以上;所述瓷砖的制备方法简单,一次烧成,有利于砖坯、面釉层、金属干粒釉层的同时成熟,有利于中间层的形成,提高瓷砖的刚性。
Metal dry granular glaze, matte metallic luster ceramic tile and preparation method of matte metallic luster ceramic tile
一种金属干粒釉料、哑光金属光泽瓷砖及其制备方法
ZHONG HUALONG (Autor:in) / LIANG YONG (Autor:in)
30.10.2020
Patent
Elektronische Ressource
Chinesisch
Production process of ceramic tile with metallic luster, ceramic tile and metal dry granular glaze
Europäisches Patentamt | 2020
|Preparation method of ceramic tile with metallic luster and ceramic tile
Europäisches Patentamt | 2023
|Ceramic tile with metallic luster and preparation method thereof
Europäisches Patentamt | 2024
|Dry granular glaze, matte ceramic tile and preparation method of dry granular glaze
Europäisches Patentamt | 2023
|Fine matte dry granular glaze ceramic tile and preparation method thereof
Europäisches Patentamt | 2023
|