Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Geopolymer cementing material for temporary spray anchor support engineering and preparation method of geopolymer cementing material
The invention relates to a geopolymer cementing material for temporary spray anchor support engineering and a preparation method of the material, the geopolymer cementing material is mainly prepared by mixing raw materials of low-calcium fly ash, granulated blast furnace slag powder and an alkali activator, the alkali activator is prepared by blending sodium silicate, sodium hydroxide or potassiumhydroxide and water, the molar ratio of M2O to SiO2 in the alkali activator is 0.50-0.78, and M represents Na or K. The invention also comprises a preparation method of the geopolymer cementing material. At normal temperature, the geopolymer cementing material disclosed by the invention can be quickly condensed and cured and can generate strength. The material provided by the invention is especially suitable for temporary slope support engineering and other similar cementing materials needing rapid strength acquisition, and has the advantages of early strength, rapid hardening, simple configuration, greenness and environmental protection.
一种用于临时性喷锚支护工程的地聚物胶凝材料及其制备方法,该地聚物胶凝材料主要由原料低钙粉煤灰、粒化高炉矿渣粉、碱活化剂混配制成,所述碱活化剂由水玻璃与氢氧化钠或氢氧化钾和水调制而成,所述碱活化剂中,M2O与SiO2的摩尔比为0.50~0.78,M代表Na或K。本发明还包括所述地聚物胶凝材料的制备方法。在常温下,本发明地聚物胶凝材料可以快速凝结固化并产生强度。本发明材料特别适用于临时性边坡支护工程等类似需要快速取得强度的胶凝材料,具有早强快硬、配置简单、绿色环保的优点。
Geopolymer cementing material for temporary spray anchor support engineering and preparation method of geopolymer cementing material
The invention relates to a geopolymer cementing material for temporary spray anchor support engineering and a preparation method of the material, the geopolymer cementing material is mainly prepared by mixing raw materials of low-calcium fly ash, granulated blast furnace slag powder and an alkali activator, the alkali activator is prepared by blending sodium silicate, sodium hydroxide or potassiumhydroxide and water, the molar ratio of M2O to SiO2 in the alkali activator is 0.50-0.78, and M represents Na or K. The invention also comprises a preparation method of the geopolymer cementing material. At normal temperature, the geopolymer cementing material disclosed by the invention can be quickly condensed and cured and can generate strength. The material provided by the invention is especially suitable for temporary slope support engineering and other similar cementing materials needing rapid strength acquisition, and has the advantages of early strength, rapid hardening, simple configuration, greenness and environmental protection.
一种用于临时性喷锚支护工程的地聚物胶凝材料及其制备方法,该地聚物胶凝材料主要由原料低钙粉煤灰、粒化高炉矿渣粉、碱活化剂混配制成,所述碱活化剂由水玻璃与氢氧化钠或氢氧化钾和水调制而成,所述碱活化剂中,M2O与SiO2的摩尔比为0.50~0.78,M代表Na或K。本发明还包括所述地聚物胶凝材料的制备方法。在常温下,本发明地聚物胶凝材料可以快速凝结固化并产生强度。本发明材料特别适用于临时性边坡支护工程等类似需要快速取得强度的胶凝材料,具有早强快硬、配置简单、绿色环保的优点。
Geopolymer cementing material for temporary spray anchor support engineering and preparation method of geopolymer cementing material
用于临时性喷锚支护工程的地聚物胶凝材料及其制备方法
CHEN WEIQUAN (Autor:in) / OUYANG SHUNTIAN (Autor:in) / LUO NENG (Autor:in) / ZHU WENFENG (Autor:in)
01.01.2021
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Preparation method of zeolite geopolymer cementing material
Europäisches Patentamt | 2020
|Europäisches Patentamt | 2021
|Carbonization curing method of geopolymer cementing material
Europäisches Patentamt | 2022
|Europäisches Patentamt | 2021
|CNF reinforced metakaolin-based geopolymer cementing material
Europäisches Patentamt | 2020
|