Early high-strength self-leveling bridge pier column reinforcing mortar material
A disclosed early-strength self-leveling bridge pier column reinforcing mortar material is prepared from the following components in parts by weight: 69 to 71 parts of quick-hardening sulphoaluminatecement, 6 to 8 parts of ordinary Portland cement, 18 parts of fly ash, 5 to 8 parts of silica fume, 2 parts of gypsum, 120 parts of quartz sand, 0.30 to 0.55 part of water reducing agent, 0.01 part ofdefoaming agent, 1 part of expanding agent, 0.005 part of SPA, 0.035 to 0.04 part of adelayed coagulant, and 2 parts of glue powder. A finished product/water equals 25/3.5-25/3.8. The material of invention has the characteristics of high early strength, stable increase of later strength, good fluidity, high bonding strength and the like, and has excellent construction performance.
本发明公开了一种早高强自流平桥梁墩柱加固砂浆材料,按重量份计包括如下组分:快硬硫铝酸盐水泥69~71份,普通硅酸盐水泥6~8份,粉煤灰18份,硅灰5~8份,石膏2份,石英砂120份,减水剂0.30~0.55份,消泡剂0.01份,膨胀剂1份,SPA 0.005份,缓凝剂0.035~0.04份,胶粉2份,成品/水=25/3.5~25/3.8。本发明具有早期强度高、后期强度稳定增长、流动性好、粘结强度高等特点,具有优良的施工性能。
Early high-strength self-leveling bridge pier column reinforcing mortar material
A disclosed early-strength self-leveling bridge pier column reinforcing mortar material is prepared from the following components in parts by weight: 69 to 71 parts of quick-hardening sulphoaluminatecement, 6 to 8 parts of ordinary Portland cement, 18 parts of fly ash, 5 to 8 parts of silica fume, 2 parts of gypsum, 120 parts of quartz sand, 0.30 to 0.55 part of water reducing agent, 0.01 part ofdefoaming agent, 1 part of expanding agent, 0.005 part of SPA, 0.035 to 0.04 part of adelayed coagulant, and 2 parts of glue powder. A finished product/water equals 25/3.5-25/3.8. The material of invention has the characteristics of high early strength, stable increase of later strength, good fluidity, high bonding strength and the like, and has excellent construction performance.
本发明公开了一种早高强自流平桥梁墩柱加固砂浆材料,按重量份计包括如下组分:快硬硫铝酸盐水泥69~71份,普通硅酸盐水泥6~8份,粉煤灰18份,硅灰5~8份,石膏2份,石英砂120份,减水剂0.30~0.55份,消泡剂0.01份,膨胀剂1份,SPA 0.005份,缓凝剂0.035~0.04份,胶粉2份,成品/水=25/3.5~25/3.8。本发明具有早期强度高、后期强度稳定增长、流动性好、粘结强度高等特点,具有优良的施工性能。
Early high-strength self-leveling bridge pier column reinforcing mortar material
一种早高强自流平桥梁墩柱加固砂浆材料
WU LAIDI (Autor:in) / WEI DINGBANG (Autor:in) / LI XIAOMIN (Autor:in) / REN GUOBIN (Autor:in) / ZHANG FUKUI (Autor:in) / YANG XIAOSEN (Autor:in) / YU XIAOLONG (Autor:in)
09.02.2021
Patent
Elektronische Ressource
Chinesisch
Bridge single-column pier reinforcing construction method
Europäisches Patentamt | 2021
|Process for reinforcing pier body of single-column pier of bridge
Europäisches Patentamt | 2021
|