Autoclaved aerated concrete B05-grade waterproof building block and preparation method thereof
The invention relates to an autoclaved aerated concrete B05-grade waterproof building block which is composed of 300-320 kg of lime, 470-510 kg of cement, 1250-1280 kg of mortar, 400-460 kg of waste slurry, 1.7-1.8 kg of aluminum powder, 15 kg of admixture 1, 0.3 kg of admixture 2 and 0.5 kg of admixture 3 according to a 5-cube mold.
本发明涉及蒸压加气混凝土B05级防水砌块,按照5立方模具计,所述防水砌块由300~320公斤的石灰、470~510公斤的水泥、1250~1280公斤的砂浆、400~460公斤的废浆、1.7~1.8公斤的铝粉、15公斤的外加剂1、0.3公斤的外加剂2以及0.5公斤的外加剂3组成。
Autoclaved aerated concrete B05-grade waterproof building block and preparation method thereof
The invention relates to an autoclaved aerated concrete B05-grade waterproof building block which is composed of 300-320 kg of lime, 470-510 kg of cement, 1250-1280 kg of mortar, 400-460 kg of waste slurry, 1.7-1.8 kg of aluminum powder, 15 kg of admixture 1, 0.3 kg of admixture 2 and 0.5 kg of admixture 3 according to a 5-cube mold.
本发明涉及蒸压加气混凝土B05级防水砌块,按照5立方模具计,所述防水砌块由300~320公斤的石灰、470~510公斤的水泥、1250~1280公斤的砂浆、400~460公斤的废浆、1.7~1.8公斤的铝粉、15公斤的外加剂1、0.3公斤的外加剂2以及0.5公斤的外加剂3组成。
Autoclaved aerated concrete B05-grade waterproof building block and preparation method thereof
蒸压加气混凝土B05级防水砌块及其制备方法
HE TIEMING (Autor:in) / XIANG JIANYONG (Autor:in) / CAO XIAOBO (Autor:in)
26.02.2021
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Preparation method of autoclaved aerated concrete block and autoclaved aerated concrete block
Europäisches Patentamt | 2021
|Autoclaved aerated concrete building block and preparation method thereof