Smooth glazed tile and production process thereof
The invention discloses and provides a smooth glazed tile with a flat and smooth surface and a production process of the smooth glazed tile. The smooth glazed tile comprises a tile body, high-temperature ground coat and surface coat are sequentially sprayed outside the tile body, and the high-temperature ground coat comprises, by percentage, 37%-50% of potassium feldspar, 1%-8% of zirconium silicate, 10%-15% of kaolin, 13%-18% of quartz, 1%-5% of calcined talc, 10%-13% of black mud powder and 3%-8% of aluminum oxide. And the surface glaze comprises the following components in percentage: 40%-55% of potassium feldspar, 18%-25% of calcite, 7%-13% of calcined talc, 5%-17% of zirconium silicate, 1%-10% of quartz, 8%-10% of black mud powder and 1%-5% of aluminum oxide. The method is suitable for the field of production and processing of smooth glazed tiles.
本发明公开并提供了一种表面平整光滑的平滑釉面砖及其生产工艺。本发明中的平滑釉面砖,包括砖体,所述砖体外依次施喷有高温底釉以及面釉,所述高温底釉按百分比算,包含以下组分:钾长石37%‑50%,硅酸锆1%‑8%,高岭土10%‑15%,石英13%‑18%,烧滑石1%‑5%,黑泥粉10%‑13%,氧化铝3%‑8%;所述面釉按百分比算,包含以下组分:钾长石40%‑55%,方解石18%‑25%,烧滑石7%‑13%,硅酸锆5%‑17%,石英1%‑10%,黑泥粉8%‑10%,氧化铝1%‑5%。本发明适用于平滑釉面砖的生产加工领域。
Smooth glazed tile and production process thereof
The invention discloses and provides a smooth glazed tile with a flat and smooth surface and a production process of the smooth glazed tile. The smooth glazed tile comprises a tile body, high-temperature ground coat and surface coat are sequentially sprayed outside the tile body, and the high-temperature ground coat comprises, by percentage, 37%-50% of potassium feldspar, 1%-8% of zirconium silicate, 10%-15% of kaolin, 13%-18% of quartz, 1%-5% of calcined talc, 10%-13% of black mud powder and 3%-8% of aluminum oxide. And the surface glaze comprises the following components in percentage: 40%-55% of potassium feldspar, 18%-25% of calcite, 7%-13% of calcined talc, 5%-17% of zirconium silicate, 1%-10% of quartz, 8%-10% of black mud powder and 1%-5% of aluminum oxide. The method is suitable for the field of production and processing of smooth glazed tiles.
本发明公开并提供了一种表面平整光滑的平滑釉面砖及其生产工艺。本发明中的平滑釉面砖,包括砖体,所述砖体外依次施喷有高温底釉以及面釉,所述高温底釉按百分比算,包含以下组分:钾长石37%‑50%,硅酸锆1%‑8%,高岭土10%‑15%,石英13%‑18%,烧滑石1%‑5%,黑泥粉10%‑13%,氧化铝3%‑8%;所述面釉按百分比算,包含以下组分:钾长石40%‑55%,方解石18%‑25%,烧滑石7%‑13%,硅酸锆5%‑17%,石英1%‑10%,黑泥粉8%‑10%,氧化铝1%‑5%。本发明适用于平滑釉面砖的生产加工领域。
Smooth glazed tile and production process thereof
一种平滑釉面砖及其生产工艺
LIANG HONGWU (Autor:in)
12.03.2021
Patent
Elektronische Ressource
Chinesisch
Stain-resistant glazed tile and production process thereof
Europäisches Patentamt | 2021
|high-gloss glazed tile and production process thereof
Europäisches Patentamt | 2021
|Thin broken crack glazed tile and production process thereof
Europäisches Patentamt | 2021
|