Animal fiber greening brick and preparation method thereof
The invention provides an animal fiber greening brick, which is prepared from animal fibers, corn stalks, white clay, a thickener, a wet strength agent, amino acid, ferrous sulfate, magnesium sulfate and borax, wherein the animal fibers comprise the following components in parts by weight: 55-65 parts of animal manure, 60-70 parts of an alkali liquor, 5-8 parts of a disinfectant, 8-12 parts of a suspending agent and 10-13 parts of a bleaching agent, the weight part ratio of the corn stalks to the animal fiber is 6-8:1, the white clay accounts for 5-8 parts by weight, the thickener accounts for 0.6-1.6 parts by weight, the wet strength agent accounts for 2-4 parts by weight, the amino acid accounts for 0.6-0.9 part by weight, the ferrous sulfate accounts for 0.1-0.2 part by weight, the magnesium sulfate accounts for 0.05-0.08 part by weight, and the borax accounts for 0.3-0.6 part by weight. According to the invention, the brick body is prepared by mixing the fibers extracted from the animal manure with the crop stalks, so that the cost is low, the preparation process is simple, energy-saving and environment-friendly, the performance is excellent, the strategic thought of sustainable development is met, and resources are utilized to the maximum extent.
本发明提供一种动物纤维绿化砖,所述动物纤维绿化砖由动物纤维、玉米秸秆、白土、增稠剂、湿强剂、氨基酸、硫矾、硫酸镁和硼砂制得,其中,所述动物纤维按重量份,由动物粪便55‑65份、碱液60‑70份、消毒剂5‑8份、悬浮剂8‑12份和漂白剂10‑13份制作而成;所述玉米秸秆与所述动物纤维按重量份数比为6‑8:1;所述白土5‑8重量份、所述增稠剂0.6‑1.6重量份、湿强剂2‑4重量份、氨基酸0.6‑0.9重量份、硫矾0.1‑0.2重量份、硫酸镁0.05‑0.08重量份、硼砂0.3‑0.6重量份。本发明采用从动物粪便中提取纤维与农作物秸秆混合制成砖体,不但成本低廉,制备工艺简单,节能环保,性能优异,同时符合可持续化发展的战略思想,最大限度的利用资源。
Animal fiber greening brick and preparation method thereof
The invention provides an animal fiber greening brick, which is prepared from animal fibers, corn stalks, white clay, a thickener, a wet strength agent, amino acid, ferrous sulfate, magnesium sulfate and borax, wherein the animal fibers comprise the following components in parts by weight: 55-65 parts of animal manure, 60-70 parts of an alkali liquor, 5-8 parts of a disinfectant, 8-12 parts of a suspending agent and 10-13 parts of a bleaching agent, the weight part ratio of the corn stalks to the animal fiber is 6-8:1, the white clay accounts for 5-8 parts by weight, the thickener accounts for 0.6-1.6 parts by weight, the wet strength agent accounts for 2-4 parts by weight, the amino acid accounts for 0.6-0.9 part by weight, the ferrous sulfate accounts for 0.1-0.2 part by weight, the magnesium sulfate accounts for 0.05-0.08 part by weight, and the borax accounts for 0.3-0.6 part by weight. According to the invention, the brick body is prepared by mixing the fibers extracted from the animal manure with the crop stalks, so that the cost is low, the preparation process is simple, energy-saving and environment-friendly, the performance is excellent, the strategic thought of sustainable development is met, and resources are utilized to the maximum extent.
本发明提供一种动物纤维绿化砖,所述动物纤维绿化砖由动物纤维、玉米秸秆、白土、增稠剂、湿强剂、氨基酸、硫矾、硫酸镁和硼砂制得,其中,所述动物纤维按重量份,由动物粪便55‑65份、碱液60‑70份、消毒剂5‑8份、悬浮剂8‑12份和漂白剂10‑13份制作而成;所述玉米秸秆与所述动物纤维按重量份数比为6‑8:1;所述白土5‑8重量份、所述增稠剂0.6‑1.6重量份、湿强剂2‑4重量份、氨基酸0.6‑0.9重量份、硫矾0.1‑0.2重量份、硫酸镁0.05‑0.08重量份、硼砂0.3‑0.6重量份。本发明采用从动物粪便中提取纤维与农作物秸秆混合制成砖体,不但成本低廉,制备工艺简单,节能环保,性能优异,同时符合可持续化发展的战略思想,最大限度的利用资源。
Animal fiber greening brick and preparation method thereof
一种动物纤维绿化砖及其制备方法
ZHOU WEIXIANG (Autor:in) / WANG XIYANG (Autor:in)
06.04.2021
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Manufacturing method of construction waste greening ecological brick
Europäisches Patentamt | 2024
|FULL-FIBER BURNER BRICK AND PREPARATION METHOD THEREOF
Europäisches Patentamt | 2022
|High-wear-resistance artificial fiber greening lawn and preparation method thereof
Europäisches Patentamt | 2024
|