Non-autoclaved aerated brick and preparation method thereof
The invention discloses a non-autoclaved aerated brick which comprises the following components in parts by weight: 2200-2400 parts of fly ash, 1400-1700 parts of weathered sand, 1100-1200 parts of mineral tailing powder, 430-450 parts of ordinary cement, 220-240 parts of water and 43-45 parts of an additive, and further discloses a preparation method of the aerated brick, comprising the following steps: mixing the fly ash, the weathered sand and the mineral tailing powder and pulping; the slurry is pumped into a pouring machine, cement and various additives are added, waste is fully utilized, the environment is protected, high-temperature autoclaving is not needed, energy consumption is low, and the prepared aerated brick is high in strength and more stable in product performance.
本发明公开了一种免蒸加气砖,以重量份计,包括以下组分:粉煤灰2200‑2400份,风化砂1400‑1700份,矿尾粉1100‑1200份,普通水泥430‑450份,水220‑240份,添加剂43‑45份,本发明还公开了该加气砖的制备方法,将粉煤灰,风化砂,矿尾粉混合并制浆,再抽取浆料至浇筑机中添加水泥及各组添加剂,充分利用废弃物,保护环境,无需高温蒸压,能耗低,制得加气砖强度高,产品性能更加稳定。
Non-autoclaved aerated brick and preparation method thereof
The invention discloses a non-autoclaved aerated brick which comprises the following components in parts by weight: 2200-2400 parts of fly ash, 1400-1700 parts of weathered sand, 1100-1200 parts of mineral tailing powder, 430-450 parts of ordinary cement, 220-240 parts of water and 43-45 parts of an additive, and further discloses a preparation method of the aerated brick, comprising the following steps: mixing the fly ash, the weathered sand and the mineral tailing powder and pulping; the slurry is pumped into a pouring machine, cement and various additives are added, waste is fully utilized, the environment is protected, high-temperature autoclaving is not needed, energy consumption is low, and the prepared aerated brick is high in strength and more stable in product performance.
本发明公开了一种免蒸加气砖,以重量份计,包括以下组分:粉煤灰2200‑2400份,风化砂1400‑1700份,矿尾粉1100‑1200份,普通水泥430‑450份,水220‑240份,添加剂43‑45份,本发明还公开了该加气砖的制备方法,将粉煤灰,风化砂,矿尾粉混合并制浆,再抽取浆料至浇筑机中添加水泥及各组添加剂,充分利用废弃物,保护环境,无需高温蒸压,能耗低,制得加气砖强度高,产品性能更加稳定。
Non-autoclaved aerated brick and preparation method thereof
一种免蒸加气砖及其制备方法
CHEN ZHENGLONG (Autor:in)
09.04.2021
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Autoclaved aerated brick and preparation method thereof
Europäisches Patentamt | 2021
|Autoclaved aerated concrete brick and preparation method thereof
Europäisches Patentamt | 2015
|Autoclaved aerated lime brick and preparation method thereof
Europäisches Patentamt | 2016
|Autoclaved aerated sand brick and preparation method thereof
Europäisches Patentamt | 2016
|