Anti-radiation ceramic tile adhesive mortar and preparation method thereof
The invention relates to anti-radiation ceramic tile adhesive mortar and a preparation method thereof, and the anti-radiation ceramic tile adhesive mortar is mainly prepared from the following components in parts by weight: a filler comprises 15.0-30.0 parts of barium sulfate sand of 40-70 meshes and 10.0-40.0 parts of other fillers. The anti-radiation ceramic tile adhesive mortar overcomes the defects that ceramic tile adhesive mortar has excellent cohesiveness, cracking resistance, hollowing resistance and aging resistance, is low in price and does not have radiation resistance, cement and redispersible latex powder are used as adhesive materials, graded sand and barium sulfate sand with the preferable mesh number are used as fillers, functional material modified carbon powder with an anti-radiation function is added, and the barium sulfate sand and the anti-radiation functional material modified carbon powder are combined and matched with other preferable components and the dosage proportion thereof, so that the anti-radiation coating has excellent anti-radiation performance.
本发明涉及一种防辐射瓷砖粘结砂浆及其制备方法,主要由以下组分按照以下重量份数比制备而成:其中,所述填料包括15.0‑30.0份的40‑70目的硫酸钡砂和10.0‑40.0份的其他填料。该发明克服了瓷砖粘结砂浆具有优良的粘结性、抗开裂性、抗空鼓性能、耐老化性能,且价格低廉,但其不具有防辐射性能的缺点,以水泥与可再分散乳胶粉为粘结材料,以级配砂和优选目数的硫酸钡砂为填料,添加具有防辐射功能的功能材料改性碳粉,通过硫酸钡砂和防辐射功能材料改性碳粉相结合,与其他优选组分及其用量比例配合,具有优异的防辐射性。
Anti-radiation ceramic tile adhesive mortar and preparation method thereof
The invention relates to anti-radiation ceramic tile adhesive mortar and a preparation method thereof, and the anti-radiation ceramic tile adhesive mortar is mainly prepared from the following components in parts by weight: a filler comprises 15.0-30.0 parts of barium sulfate sand of 40-70 meshes and 10.0-40.0 parts of other fillers. The anti-radiation ceramic tile adhesive mortar overcomes the defects that ceramic tile adhesive mortar has excellent cohesiveness, cracking resistance, hollowing resistance and aging resistance, is low in price and does not have radiation resistance, cement and redispersible latex powder are used as adhesive materials, graded sand and barium sulfate sand with the preferable mesh number are used as fillers, functional material modified carbon powder with an anti-radiation function is added, and the barium sulfate sand and the anti-radiation functional material modified carbon powder are combined and matched with other preferable components and the dosage proportion thereof, so that the anti-radiation coating has excellent anti-radiation performance.
本发明涉及一种防辐射瓷砖粘结砂浆及其制备方法,主要由以下组分按照以下重量份数比制备而成:其中,所述填料包括15.0‑30.0份的40‑70目的硫酸钡砂和10.0‑40.0份的其他填料。该发明克服了瓷砖粘结砂浆具有优良的粘结性、抗开裂性、抗空鼓性能、耐老化性能,且价格低廉,但其不具有防辐射性能的缺点,以水泥与可再分散乳胶粉为粘结材料,以级配砂和优选目数的硫酸钡砂为填料,添加具有防辐射功能的功能材料改性碳粉,通过硫酸钡砂和防辐射功能材料改性碳粉相结合,与其他优选组分及其用量比例配合,具有优异的防辐射性。
Anti-radiation ceramic tile adhesive mortar and preparation method thereof
防辐射瓷砖粘结砂浆及其制备方法
JIANG KEFEI (Autor:in) / LI XIAOLIANG (Autor:in) / ZHANG SHAOYU (Autor:in) / YANG SHUAI (Autor:in)
17.09.2021
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Ceramic tile paving mortar and preparation method thereof
Europäisches Patentamt | 2024
|Gypsum-based ground tile adhesive mortar and preparation method thereof
Europäisches Patentamt | 2022
|