The invention discloses waterproof anti-crack environment-friendly mortar and a preparation method thereof. The mortar is prepared from the following components in parts by weight: 250 to 500 parts of cement; 5-50 parts of silica fume; 20-60 parts of an expanding agent; 100-200 parts of quartz sand with a particle size of 40 to 70 mesh; 200-300 parts of quartz sand with a particle size of 70 to 120 mesh; 100-300 parts of 200-mesh quartz sand; 0.03-0.05 part of a polycarboxylic acid water reducing agent; 5-30 parts of redispersible latex powder; 1-10 parts of polyvinyl alcohol fiber; 1-6 parts of cellulose fiber; 1-5 parts of wood fiber; 1-3 parts of polypropylene short fiber; 1-8 parts of a water repellent; and 2-10 parts of an anti-permeability agent. The mortar has good anti-cracking performance and anti-seepage performance.
本发明公开了一种防水抗裂环保砂浆及其制备方法。以各组分的重量份数计,所述砂浆包括以下组分:水泥:250‑500;微硅粉:5‑50;膨胀剂:20‑60;40‑70姆石英砂:100‑200;70‑120姆石英砂:200‑300;200姆石英砂:100‑300;聚羧酸减水剂:0.03‑0.05;可再分散乳胶粉:5‑30;聚乙烯醇纤维:1‑10;纤维素纤维:1‑6;木质纤维:1‑5;聚丙烯短纤维:1‑3;憎水剂:1‑8;抗渗剂:2‑10。所述砂浆具有良好的抗裂性能和抗渗性能。
The invention discloses waterproof anti-crack environment-friendly mortar and a preparation method thereof. The mortar is prepared from the following components in parts by weight: 250 to 500 parts of cement; 5-50 parts of silica fume; 20-60 parts of an expanding agent; 100-200 parts of quartz sand with a particle size of 40 to 70 mesh; 200-300 parts of quartz sand with a particle size of 70 to 120 mesh; 100-300 parts of 200-mesh quartz sand; 0.03-0.05 part of a polycarboxylic acid water reducing agent; 5-30 parts of redispersible latex powder; 1-10 parts of polyvinyl alcohol fiber; 1-6 parts of cellulose fiber; 1-5 parts of wood fiber; 1-3 parts of polypropylene short fiber; 1-8 parts of a water repellent; and 2-10 parts of an anti-permeability agent. The mortar has good anti-cracking performance and anti-seepage performance.
本发明公开了一种防水抗裂环保砂浆及其制备方法。以各组分的重量份数计,所述砂浆包括以下组分:水泥:250‑500;微硅粉:5‑50;膨胀剂:20‑60;40‑70姆石英砂:100‑200;70‑120姆石英砂:200‑300;200姆石英砂:100‑300;聚羧酸减水剂:0.03‑0.05;可再分散乳胶粉:5‑30;聚乙烯醇纤维:1‑10;纤维素纤维:1‑6;木质纤维:1‑5;聚丙烯短纤维:1‑3;憎水剂:1‑8;抗渗剂:2‑10。所述砂浆具有良好的抗裂性能和抗渗性能。
Waterproof anti-crack cement mortar and preparation method thereof
Europäisches Patentamt | 2024
|Macromolecular anti-crack waterproof mortar and preparation method thereof
Europäisches Patentamt | 2021
|Plastering anti-crack waterproof mortar and preparation method thereof
Europäisches Patentamt | 2020
|Waterproof heat insulation environment-friendly mortar and preparation method thereof
Europäisches Patentamt | 2015
|