Retro brick prepared based on steel slag carbonization and preparation method thereof
The invention discloses a retro brick prepared based on steel slag carbonization and a preparation method thereof, and the retro brick prepared based on steel slag carbonization is prepared from the following raw materials by mass: 35-50 parts of steel slag, 20-35 parts of quartz sand, 10-20 parts of gamma-C2S powder, 5-20 parts of fly ash, and 5-10 parts of water. The strength performance of the prepared retro brick is remarkably improved by performing carbonization treatment on the steel slag and cooperating with the hydration reaction of the fly ash; the steel slag and fly ash are used as raw materials, the materials are widely available, the production process is simple, the preparation cost is remarkably reduced, and the preparation efficiency is improved.
本发明公开了一种基于钢渣碳化制备的复古砖及其制备方法,以质量份数计,所述基于钢渣碳化制备的复古砖由如下组分原料制成:钢渣35~50份,石英砂20~35份,γ‑C2S粉体10~20份,粉煤灰5~20份,以及水5~10份。本发明通过对钢渣进行碳化处理,并配合粉煤灰水化反应,所制备复古砖的强度性能显著提升;以钢渣和粉煤灰为原料,取材广泛,生产工艺简单,显著降低了制备成本,提升了制备效率。
Retro brick prepared based on steel slag carbonization and preparation method thereof
The invention discloses a retro brick prepared based on steel slag carbonization and a preparation method thereof, and the retro brick prepared based on steel slag carbonization is prepared from the following raw materials by mass: 35-50 parts of steel slag, 20-35 parts of quartz sand, 10-20 parts of gamma-C2S powder, 5-20 parts of fly ash, and 5-10 parts of water. The strength performance of the prepared retro brick is remarkably improved by performing carbonization treatment on the steel slag and cooperating with the hydration reaction of the fly ash; the steel slag and fly ash are used as raw materials, the materials are widely available, the production process is simple, the preparation cost is remarkably reduced, and the preparation efficiency is improved.
本发明公开了一种基于钢渣碳化制备的复古砖及其制备方法,以质量份数计,所述基于钢渣碳化制备的复古砖由如下组分原料制成:钢渣35~50份,石英砂20~35份,γ‑C2S粉体10~20份,粉煤灰5~20份,以及水5~10份。本发明通过对钢渣进行碳化处理,并配合粉煤灰水化反应,所制备复古砖的强度性能显著提升;以钢渣和粉煤灰为原料,取材广泛,生产工艺简单,显著降低了制备成本,提升了制备效率。
Retro brick prepared based on steel slag carbonization and preparation method thereof
一种基于钢渣碳化制备的复古砖及其制备方法
CAI YINGHUI (Autor:in) / ZHANG XUELEI (Autor:in) / LI JUNCHEN (Autor:in) / MA YUNSHENG (Autor:in) / CUI DONGBO (Autor:in) / ZHAO DU (Autor:in)
21.01.2022
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Europäisches Patentamt | 2023
|Europäisches Patentamt | 2022
|Slag line brick, preparation method thereof and application of slag line brick in steel ladle
Europäisches Patentamt | 2024
|Method for preparing building brick through direct slag carbonization
Europäisches Patentamt | 2015
|Black road brick prepared from steel slag and preparation method of black road brick
Europäisches Patentamt | 2021
|