Environment-friendly building wall material and processing technology
The invention discloses an environment-friendly building wall material and a processing technology, the formula comprises attapulgite, sepiolite, tourmaline, nano titanium dioxide, activated carbon, diatom ooze, kaolin, plant fiber, an ultraviolet light absorber, an organic nitrogen flame retardant, a phosphorus flame retardant and aerogel, the processing technology comprises the following steps: 1, preparing raw materials; step 2, preparing a decomposing agent; step 3, manufacturing wall materials; step 4, filling and storing; in the third step, the temperature of the reaction kettle is controlled to be 100-150 DEG C, and the reaction time is 0.5-2 h. Compared with an existing building wall material and a processing technology, the environment-friendly performance of the material is improved by adding the attapulgite, the sepiolite, the tourmaline and the nano titanium dioxide; by adding the aerogel, the organic nitrogen flame retardant and the phosphorus flame retardant, the fireproof and weather-resistant properties of the material are enhanced; by adding the aerogel, the kaolin and the plant fibers, the light capacity and the high strength of the material are ensured at the same time.
本发明公开了一种环保型建筑墙体材料及加工工艺,配方包括:凹凸棒土、海泡石、电气石、纳米二氧化钛、活性炭、硅藻泥、高岭土、植物纤维、紫外线吸收剂、有机氮系阻燃剂、磷系阻燃剂和气凝胶,步骤包括步骤一,准备原料;步骤二,制作分解剂;步骤三,制作墙材;步骤四,灌装保存;所述步骤三中反应釜温度控制为100‑150℃,反应时间为0.5‑2h,本发明相较于现有的建筑墙体材料及加工工艺,通过增加凹凸棒土、海泡石、电气石、纳米二氧化钛,增加了材料的环保性能;本发明通过增加气凝胶、机氮系阻燃剂、磷系阻燃剂,增强了材料的防火耐候性;本发明通过气凝胶、高岭土、植物纤维的加入,同时保证了材料的轻容量和高强度。
Environment-friendly building wall material and processing technology
The invention discloses an environment-friendly building wall material and a processing technology, the formula comprises attapulgite, sepiolite, tourmaline, nano titanium dioxide, activated carbon, diatom ooze, kaolin, plant fiber, an ultraviolet light absorber, an organic nitrogen flame retardant, a phosphorus flame retardant and aerogel, the processing technology comprises the following steps: 1, preparing raw materials; step 2, preparing a decomposing agent; step 3, manufacturing wall materials; step 4, filling and storing; in the third step, the temperature of the reaction kettle is controlled to be 100-150 DEG C, and the reaction time is 0.5-2 h. Compared with an existing building wall material and a processing technology, the environment-friendly performance of the material is improved by adding the attapulgite, the sepiolite, the tourmaline and the nano titanium dioxide; by adding the aerogel, the organic nitrogen flame retardant and the phosphorus flame retardant, the fireproof and weather-resistant properties of the material are enhanced; by adding the aerogel, the kaolin and the plant fibers, the light capacity and the high strength of the material are ensured at the same time.
本发明公开了一种环保型建筑墙体材料及加工工艺,配方包括:凹凸棒土、海泡石、电气石、纳米二氧化钛、活性炭、硅藻泥、高岭土、植物纤维、紫外线吸收剂、有机氮系阻燃剂、磷系阻燃剂和气凝胶,步骤包括步骤一,准备原料;步骤二,制作分解剂;步骤三,制作墙材;步骤四,灌装保存;所述步骤三中反应釜温度控制为100‑150℃,反应时间为0.5‑2h,本发明相较于现有的建筑墙体材料及加工工艺,通过增加凹凸棒土、海泡石、电气石、纳米二氧化钛,增加了材料的环保性能;本发明通过增加气凝胶、机氮系阻燃剂、磷系阻燃剂,增强了材料的防火耐候性;本发明通过气凝胶、高岭土、植物纤维的加入,同时保证了材料的轻容量和高强度。
Environment-friendly building wall material and processing technology
一种环保型建筑墙体材料及加工工艺
CHU YANJUN (Autor:in)
21.01.2022
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Building outer wall environment-friendly material spraying device
Europäisches Patentamt | 2022
|