The invention provides a curing method of a high-efficiency soft porcelain flexible facing brick. The curing method comprises the following steps: 1, preparing a mixed emulsion; 2, preparing mixed powder; 3, adding the mixed emulsion into the mixed powder, adding 5-15 parts of water, and stirring to obtain soft porcelain slurry; 4, injecting the slurry in the step 3 into a mold; and 5, curing. Wherein the curing step comprises microwave curing treatment, meanwhile, due to the fact that a certain temperature exists on the outer layer of the soft porcelain slurry, the whole curing process is carried out inside and outside the soft porcelain slurry at the same time, and in order to further improve the curing efficiency, a wave absorbing agent is further added into the soft porcelain slurry, and the curing efficiency is improved.
本公开提供了一种高效软瓷柔性饰面砖的固化方法,包括如下步骤:1、混合乳液的制备;2、混合粉料的制备;3、将混合乳液加入到混合粉料中,另外5‑15份水,搅拌得到软瓷浆料;4、将步骤3中的浆料注入到模具中;5、固化。其中,固化步骤中包括微波固化处理,同时由于软瓷浆料的外层存在一定温度,因此,整个固化过程是软瓷浆料内部和外部同时进行,为了进一步的提高固化效率,在软瓷浆料中还加入了吸波剂,提高固化效率。
The invention provides a curing method of a high-efficiency soft porcelain flexible facing brick. The curing method comprises the following steps: 1, preparing a mixed emulsion; 2, preparing mixed powder; 3, adding the mixed emulsion into the mixed powder, adding 5-15 parts of water, and stirring to obtain soft porcelain slurry; 4, injecting the slurry in the step 3 into a mold; and 5, curing. Wherein the curing step comprises microwave curing treatment, meanwhile, due to the fact that a certain temperature exists on the outer layer of the soft porcelain slurry, the whole curing process is carried out inside and outside the soft porcelain slurry at the same time, and in order to further improve the curing efficiency, a wave absorbing agent is further added into the soft porcelain slurry, and the curing efficiency is improved.
本公开提供了一种高效软瓷柔性饰面砖的固化方法,包括如下步骤:1、混合乳液的制备;2、混合粉料的制备;3、将混合乳液加入到混合粉料中,另外5‑15份水,搅拌得到软瓷浆料;4、将步骤3中的浆料注入到模具中;5、固化。其中,固化步骤中包括微波固化处理,同时由于软瓷浆料的外层存在一定温度,因此,整个固化过程是软瓷浆料内部和外部同时进行,为了进一步的提高固化效率,在软瓷浆料中还加入了吸波剂,提高固化效率。
Preparation method of photovoltaic soft porcelain face brick
Europäisches Patentamt | 2022
|Europäisches Patentamt | 2020
|Flexible soft porcelain and preparation method thereof
Europäisches Patentamt | 2021
|Europäisches Patentamt | 2024
|Porcelain glazed brick prepared from waste materials and production method of porcelain glazed brick
Europäisches Patentamt | 2021
|