The invention provides a flame-retardant low-smoke rock wool composite board for a fire-fighting pipeline and a manufacturing process of the flame-retardant low-smoke rock wool composite board, and relates to the technical field of traction brackets. 4.5-5 parts of dolomite; 5-10 parts of slag; 5 to 10 parts of coke; a catalyst; 2 to 4 parts; 3-5 parts of aluminum magnesium powder; 3-5 parts of an auxiliary smoke suppressant; the graystone, the slag, the coke, the catalyst, the aluminum magnesium powder, the auxiliary smoke suppressant and the carbon-forming agent are weighed according to a specific weight part ratio, so that the content and ratio data of each raw material can be conveniently recorded, and the preparation process can be conveniently and continuously improved by preparation personnel in the later period; 70 parts of basalt, 10 parts of slag and 5 parts of coke are mixed and stirred at a high speed through a high-speed mixer. The preparation method solves the problems that rock wool produced by a traditional preparation process has the basic characteristics of heat preservation and flame resistance of rock wool, the low-smoke performance is general, more smoke is generated during combustion, the requirement for the preparation process is relatively harsh, and the preparation process is relatively tedious.
本发明提供一种消防管道用阻燃低烟岩棉复合板及其制造工艺,涉及牵引支架技术领域,由下述重量份数原料制成:玄武岩60‑70份;白云石4.5‑5份;矿渣5‑10份;焦炭5‑10份;催化剂;2‑4份;铝镁粉3‑5份;辅助抑烟剂3‑5份;成碳剂1‑2份,在对玄武石、矿渣、焦炭、催化剂、铝镁粉、辅助抑烟剂以及成碳剂按照特定重量份数配比进行称量,方便对各个原材料含量以及配比数据进行记录,进而使得制备流程可以方便制备人员后期不断进行改进,以玄武岩70份、矿渣10份和焦炭5份经高速混合机进行高速混合搅拌。本发明,解决了传统制备工艺生产出来的岩棉在具备岩棉保温耐燃的基本特性下,低烟性能一般,燃烧产生的烟雾较多,制备流程要求较为苛刻,制备流程较为繁琐的问题。
The invention provides a flame-retardant low-smoke rock wool composite board for a fire-fighting pipeline and a manufacturing process of the flame-retardant low-smoke rock wool composite board, and relates to the technical field of traction brackets. 4.5-5 parts of dolomite; 5-10 parts of slag; 5 to 10 parts of coke; a catalyst; 2 to 4 parts; 3-5 parts of aluminum magnesium powder; 3-5 parts of an auxiliary smoke suppressant; the graystone, the slag, the coke, the catalyst, the aluminum magnesium powder, the auxiliary smoke suppressant and the carbon-forming agent are weighed according to a specific weight part ratio, so that the content and ratio data of each raw material can be conveniently recorded, and the preparation process can be conveniently and continuously improved by preparation personnel in the later period; 70 parts of basalt, 10 parts of slag and 5 parts of coke are mixed and stirred at a high speed through a high-speed mixer. The preparation method solves the problems that rock wool produced by a traditional preparation process has the basic characteristics of heat preservation and flame resistance of rock wool, the low-smoke performance is general, more smoke is generated during combustion, the requirement for the preparation process is relatively harsh, and the preparation process is relatively tedious.
本发明提供一种消防管道用阻燃低烟岩棉复合板及其制造工艺,涉及牵引支架技术领域,由下述重量份数原料制成:玄武岩60‑70份;白云石4.5‑5份;矿渣5‑10份;焦炭5‑10份;催化剂;2‑4份;铝镁粉3‑5份;辅助抑烟剂3‑5份;成碳剂1‑2份,在对玄武石、矿渣、焦炭、催化剂、铝镁粉、辅助抑烟剂以及成碳剂按照特定重量份数配比进行称量,方便对各个原材料含量以及配比数据进行记录,进而使得制备流程可以方便制备人员后期不断进行改进,以玄武岩70份、矿渣10份和焦炭5份经高速混合机进行高速混合搅拌。本发明,解决了传统制备工艺生产出来的岩棉在具备岩棉保温耐燃的基本特性下,低烟性能一般,燃烧产生的烟雾较多,制备流程要求较为苛刻,制备流程较为繁琐的问题。
Flame-retardant low-smoke rock wool composite board for fire-fighting pipeline and manufacturing process of flame-retardant low-smoke rock wool composite board
一种消防管道用阻燃低烟岩棉复合板及其制造工艺
LU JIAZHI (Autor:in)
22.07.2022
Patent
Elektronische Ressource
Chinesisch
Heat-resistant and flame-retardant integrated rock wool board
Europäisches Patentamt | 2020
|Flame-retardant thermal insulation rock wool board and preparation method thereof
Europäisches Patentamt | 2024
|Europäisches Patentamt | 2021
|Fireproof flame-retardant rock wool thermal insulation material with aerogel
Europäisches Patentamt | 2022
|