Rapid structure repairing material and preparation method thereof
The invention relates to the technical field of constructional engineering materials, and discloses a rapid structure repairing material, which comprises the following raw materials by weight: 250-400 parts of compound cement, 200-450 parts of quartz sand, 200-400 parts of graded stone, 10-50 parts of a composite expanding agent, 10-30 parts of redispersible latex powder, 1-3 parts of cellulose, 1-3 parts of a binder, 1-3 parts of an adhesive, and 1-2 parts of a superplasticizer. According to the rapid structure repairing material and the preparation method thereof, the repairing material is prepared from the compound cement, the quartz sand, the graded stones, the compound expanding agent, the redispersible latex powder, the cellulose, the binding agent, the adhesive and the efficient water reducing agent, so that the overall strength of the repairing material can be effectively improved, and the overall bonding force of the repairing material can be effectively improved; the overall service life of the repairing material can be effectively prolonged, and the advantages of high strength, large bonding force and long service life are achieved.
本发明涉及建筑工程材料技术领域,且公开了一种快速结构修补料,包括以下重量份数配比的原料:复配水泥250‑400份、石英砂200‑450份、级配石子200‑400份、复合型膨胀剂10‑50份、可再分散乳胶粉10‑30份、纤维素1‑3份、结合剂1‑3份、粘接剂1‑3份、高效减水剂1‑2份。该快速结构修补料及其制备方法,通过采用复配水泥、石英砂、级配石子、复合型膨胀剂、可再分散乳胶粉、纤维素、结合剂、粘接剂、高效减水剂制得的修补料,能够有效提高修补料整体的强度,能够有效提高修补料整体的粘接力,能够有效提高修补料整体的使用寿命,达到了强度高、粘接力大和使用寿命长的优点。
Rapid structure repairing material and preparation method thereof
The invention relates to the technical field of constructional engineering materials, and discloses a rapid structure repairing material, which comprises the following raw materials by weight: 250-400 parts of compound cement, 200-450 parts of quartz sand, 200-400 parts of graded stone, 10-50 parts of a composite expanding agent, 10-30 parts of redispersible latex powder, 1-3 parts of cellulose, 1-3 parts of a binder, 1-3 parts of an adhesive, and 1-2 parts of a superplasticizer. According to the rapid structure repairing material and the preparation method thereof, the repairing material is prepared from the compound cement, the quartz sand, the graded stones, the compound expanding agent, the redispersible latex powder, the cellulose, the binding agent, the adhesive and the efficient water reducing agent, so that the overall strength of the repairing material can be effectively improved, and the overall bonding force of the repairing material can be effectively improved; the overall service life of the repairing material can be effectively prolonged, and the advantages of high strength, large bonding force and long service life are achieved.
本发明涉及建筑工程材料技术领域,且公开了一种快速结构修补料,包括以下重量份数配比的原料:复配水泥250‑400份、石英砂200‑450份、级配石子200‑400份、复合型膨胀剂10‑50份、可再分散乳胶粉10‑30份、纤维素1‑3份、结合剂1‑3份、粘接剂1‑3份、高效减水剂1‑2份。该快速结构修补料及其制备方法,通过采用复配水泥、石英砂、级配石子、复合型膨胀剂、可再分散乳胶粉、纤维素、结合剂、粘接剂、高效减水剂制得的修补料,能够有效提高修补料整体的强度,能够有效提高修补料整体的粘接力,能够有效提高修补料整体的使用寿命,达到了强度高、粘接力大和使用寿命长的优点。
Rapid structure repairing material and preparation method thereof
一种快速结构修补料及其制备方法
LI JIALIANG (Autor:in) / LU XIAOLIN (Autor:in) / ZHANG WENQIANG (Autor:in)
01.11.2022
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Rapid road repairing material and preparation method thereof
Europäisches Patentamt | 2024
|Rapid concrete repairing material and preparation method thereof
Europäisches Patentamt | 2021
|Rapid pavement repairing material and preparation method thereof
Europäisches Patentamt | 2021
|High-ductility concrete rapid structure repairing material and preparation method thereof
Europäisches Patentamt | 2023
|Concrete surface rapid repairing material and preparation method thereof
Europäisches Patentamt | 2020
|