Environment-friendly building material composition with improved early strength
The present invention relates to a building material composition comprising up to 55 dry weight% Portland cement with high early and later compressive strength. Other main components in the cement are SCM, limestone, a sulfate radical source and an accelerant.
本发明涉及具有高的早期和后期压缩强度的包含至多55干重%的波特兰水泥的建筑材料组合物。水泥中的其它主要组分为SCM、石灰石、硫酸根源和促进剂。
Environment-friendly building material composition with improved early strength
The present invention relates to a building material composition comprising up to 55 dry weight% Portland cement with high early and later compressive strength. Other main components in the cement are SCM, limestone, a sulfate radical source and an accelerant.
本发明涉及具有高的早期和后期压缩强度的包含至多55干重%的波特兰水泥的建筑材料组合物。水泥中的其它主要组分为SCM、石灰石、硫酸根源和促进剂。
Environment-friendly building material composition with improved early strength
具有改进的早期强度的环境友好的建筑材料组合物
LI XUERUN (Autor:in) / HESSE CHRISTOPH (Autor:in) / MEYER BERND (Autor:in) / BIZZOJERO JOSEPH (Autor:in)
04.11.2022
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME