The invention belongs to the technical field of building materials, and particularly relates to an energy-saving environment-friendly indoor building material and a preparation method thereof. The energy-saving environment-friendly indoor building material is specifically prepared from 2 to 4 parts of perlite, 4 to 6 parts of polyurethane foam plastic, 6 to 8 parts of gypsum, 12 to 13 parts of fine sand, 3 to 5 parts of cement, 7.5 to 8.5 parts of slag, 3 to 5 parts of diatomite, 5 to 7 parts of heat-conducting filler, 3 to 5 parts of resin, 8 to 10 parts of gravel, 6 to 7 parts of kaolin, 1.2 to 1.5 parts of retarder, 2.3 to 2.7 parts of water reducing agent, 0.8 to 1.0 part of antioxidant, 0.6 to 1.0 part of cross-linking agent and 0.3 to 0.7 part of hardening agent. The raw materials adopted by the indoor building material do not contain volatile substances, after the indoor building material is prepared into the building material, toxic substances cannot be generated to pollute the indoor air environment even if the building material is used for a long time, and the use environmental protection performance is greatly improved.
本发明属于建筑材料技术领域,具体为一种节能型环保室内建筑材料及其制备方法,该节能型环保室内建筑材料具体包括:珍珠岩2‑4份、聚氨酯泡沫塑料4‑6份、石膏6‑8份、细砂12‑13份、水泥3‑5份、矿渣7.5‑8.5份、硅藻土3‑5份、导热填料5‑7份、树脂3‑5份、碎石8‑10份、高岭土6‑7份、缓凝剂1.2‑1.5份、减水剂2.3‑2.7份、抗氧化剂0.8‑1.0份、交联剂0.6‑1.0份、硬化剂0.3‑0.7份、增稠剂0.6‑0.8份和水20‑30份,该室内建筑材料采用的原料中,不具备挥发性物质,在制备成建筑材料之后,即使长时间使用,也不会产生有毒物质污染室内空气环境,大大提高了使用环保性能。
The invention belongs to the technical field of building materials, and particularly relates to an energy-saving environment-friendly indoor building material and a preparation method thereof. The energy-saving environment-friendly indoor building material is specifically prepared from 2 to 4 parts of perlite, 4 to 6 parts of polyurethane foam plastic, 6 to 8 parts of gypsum, 12 to 13 parts of fine sand, 3 to 5 parts of cement, 7.5 to 8.5 parts of slag, 3 to 5 parts of diatomite, 5 to 7 parts of heat-conducting filler, 3 to 5 parts of resin, 8 to 10 parts of gravel, 6 to 7 parts of kaolin, 1.2 to 1.5 parts of retarder, 2.3 to 2.7 parts of water reducing agent, 0.8 to 1.0 part of antioxidant, 0.6 to 1.0 part of cross-linking agent and 0.3 to 0.7 part of hardening agent. The raw materials adopted by the indoor building material do not contain volatile substances, after the indoor building material is prepared into the building material, toxic substances cannot be generated to pollute the indoor air environment even if the building material is used for a long time, and the use environmental protection performance is greatly improved.
本发明属于建筑材料技术领域,具体为一种节能型环保室内建筑材料及其制备方法,该节能型环保室内建筑材料具体包括:珍珠岩2‑4份、聚氨酯泡沫塑料4‑6份、石膏6‑8份、细砂12‑13份、水泥3‑5份、矿渣7.5‑8.5份、硅藻土3‑5份、导热填料5‑7份、树脂3‑5份、碎石8‑10份、高岭土6‑7份、缓凝剂1.2‑1.5份、减水剂2.3‑2.7份、抗氧化剂0.8‑1.0份、交联剂0.6‑1.0份、硬化剂0.3‑0.7份、增稠剂0.6‑0.8份和水20‑30份,该室内建筑材料采用的原料中,不具备挥发性物质,在制备成建筑材料之后,即使长时间使用,也不会产生有毒物质污染室内空气环境,大大提高了使用环保性能。
Energy-saving environment-friendly indoor building material and preparation method thereof
一种节能型环保室内建筑材料及其制备方法
BAI KAI (Autor:in)
24.01.2023
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Preparation method of environment-friendly energy-saving building material
Europäisches Patentamt | 2023
|Energy-saving and environment-friendly building decoration material and preparation method thereof
Europäisches Patentamt | 2021
|