Sintering-free antique tile formula and preparation method thereof
The invention discloses a sintering-free antique tile formula and a preparation method thereof. A blank of the sintering-free antique tile is prepared from the following components in percentage by weight: 1.0%-1.3% of redispersible latex powder, 1.2%-1.5% of hydroxypropyl methyl cellulose, 0.5%-0.8% of a cement reinforcing agent, 0.4%-0.6% of a cement preservative, 0.8%-1% of a mixed clean soil sealing curing agent, 0.3%-0.6% of a water reducing agent, 0.2%-0.5% of graphene, 0.2%-0.5% of concrete fibers, 0.4%-0.7% of a defoaming agent, 0.4%-0.7% of an anti-alkali agent, 0.6%-0.8% of carbon black, 40%-50% of industrial waste, 10%-12% of fly ash and 20%-23% of cement. And 14%-17% of tap water. The invention relates to the technical field of preparation of archaized tiles. The archaized tiles produced according to the formula are free of emissions, good in environmental friendliness, high in strength, low in water absorption rate, adjustable in color and good in freeze-thaw resistance and weather resistance.
本发明公开了一种免烧结仿古瓦配方及其制备方法,免烧结仿古瓦的坯料按如下重量百分比组分组成:再分散乳胶粉1.0%‑1.3%、羟丙基甲基纤维素1.2%‑1.5%、水泥增强剂0.5%‑0.8%、水泥防腐剂0.4%‑0.6%、混净土密封固化剂0.8%‑1%、减水剂0.3%‑0.6%、石墨烯0.2%‑0.5%、混凝土纤维0.2%‑0.5%、消泡剂0.4%‑0.7%、反碱剂0.4%‑0.7%、炭黑0.6%‑0.8%、工业废弃物40%‑50%、粉煤灰10%‑12%、水泥20%‑23%、自来水14%‑17%。本发明涉及仿古瓦制备技术领域,通过本配方生产的仿古瓦没有排放物环保性好、强度高、吸水率低、颜色可调以及良好的抗冻融性和抗风化性。
Sintering-free antique tile formula and preparation method thereof
The invention discloses a sintering-free antique tile formula and a preparation method thereof. A blank of the sintering-free antique tile is prepared from the following components in percentage by weight: 1.0%-1.3% of redispersible latex powder, 1.2%-1.5% of hydroxypropyl methyl cellulose, 0.5%-0.8% of a cement reinforcing agent, 0.4%-0.6% of a cement preservative, 0.8%-1% of a mixed clean soil sealing curing agent, 0.3%-0.6% of a water reducing agent, 0.2%-0.5% of graphene, 0.2%-0.5% of concrete fibers, 0.4%-0.7% of a defoaming agent, 0.4%-0.7% of an anti-alkali agent, 0.6%-0.8% of carbon black, 40%-50% of industrial waste, 10%-12% of fly ash and 20%-23% of cement. And 14%-17% of tap water. The invention relates to the technical field of preparation of archaized tiles. The archaized tiles produced according to the formula are free of emissions, good in environmental friendliness, high in strength, low in water absorption rate, adjustable in color and good in freeze-thaw resistance and weather resistance.
本发明公开了一种免烧结仿古瓦配方及其制备方法,免烧结仿古瓦的坯料按如下重量百分比组分组成:再分散乳胶粉1.0%‑1.3%、羟丙基甲基纤维素1.2%‑1.5%、水泥增强剂0.5%‑0.8%、水泥防腐剂0.4%‑0.6%、混净土密封固化剂0.8%‑1%、减水剂0.3%‑0.6%、石墨烯0.2%‑0.5%、混凝土纤维0.2%‑0.5%、消泡剂0.4%‑0.7%、反碱剂0.4%‑0.7%、炭黑0.6%‑0.8%、工业废弃物40%‑50%、粉煤灰10%‑12%、水泥20%‑23%、自来水14%‑17%。本发明涉及仿古瓦制备技术领域,通过本配方生产的仿古瓦没有排放物环保性好、强度高、吸水率低、颜色可调以及良好的抗冻融性和抗风化性。
Sintering-free antique tile formula and preparation method thereof
一种免烧结仿古瓦配方及其制备方法
GUO YONGHONG (Autor:in)
02.06.2023
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Travertine-like antique ceramic tile and preparation method thereof
Europäisches Patentamt | 2024
|Preparation method of high-strength antique grey tile
Europäisches Patentamt | 2022
|