The invention belongs to the technical field of terrace materials, and particularly relates to a processing technology of an epoxy resin sports terrace material which is prepared from the following raw materials in parts by weight: 40-50 parts of epoxy resin, 30-35 parts of silica powder, 15-18 parts of ferric oxide, 8-12 parts of butadiene styrene rubber, 10-14 parts of clay, 0.2-0.6 part of a defoaming agent, 10-16 parts of ethylene bis stearamide and 3-5 parts of sodium gluconate. 8-14 parts of an elastic agent and 8-14 parts of a quick drying agent; the elastic agent is added into the epoxy resin terrace material, so that the elastic effect of the terrace material is improved, the movement performance of a laid site is improved, meanwhile, the curing time of the terrace material can be shortened by adding the quick-drying agent, and the laying speed of the terrace material is increased.
本发明属于地坪材料技术领域,具体的说是一种环氧树脂运动地坪材料加工工艺,该材料由下列重量份的原料组成:环氧树脂40‑50份,硅微粉30‑35份,氧化铁15‑18份,丁苯橡胶8‑12份,黏土10‑14份,消泡剂0.2‑0.6份,乙烯基双硬脂酰胺10‑16份,葡萄糖酸钠3‑5份,弹性剂8‑14份,速干剂8‑14份;在环氧树脂地坪材料中添加弹性剂,提高了地坪材料的弹性效果,使得所铺设场地的运动性能得到提升,同时速干剂的添加也能缩短地坪材料的固化时间,加快地坪材料的铺设速度。
The invention belongs to the technical field of terrace materials, and particularly relates to a processing technology of an epoxy resin sports terrace material which is prepared from the following raw materials in parts by weight: 40-50 parts of epoxy resin, 30-35 parts of silica powder, 15-18 parts of ferric oxide, 8-12 parts of butadiene styrene rubber, 10-14 parts of clay, 0.2-0.6 part of a defoaming agent, 10-16 parts of ethylene bis stearamide and 3-5 parts of sodium gluconate. 8-14 parts of an elastic agent and 8-14 parts of a quick drying agent; the elastic agent is added into the epoxy resin terrace material, so that the elastic effect of the terrace material is improved, the movement performance of a laid site is improved, meanwhile, the curing time of the terrace material can be shortened by adding the quick-drying agent, and the laying speed of the terrace material is increased.
本发明属于地坪材料技术领域,具体的说是一种环氧树脂运动地坪材料加工工艺,该材料由下列重量份的原料组成:环氧树脂40‑50份,硅微粉30‑35份,氧化铁15‑18份,丁苯橡胶8‑12份,黏土10‑14份,消泡剂0.2‑0.6份,乙烯基双硬脂酰胺10‑16份,葡萄糖酸钠3‑5份,弹性剂8‑14份,速干剂8‑14份;在环氧树脂地坪材料中添加弹性剂,提高了地坪材料的弹性效果,使得所铺设场地的运动性能得到提升,同时速干剂的添加也能缩短地坪材料的固化时间,加快地坪材料的铺设速度。
Epoxy resin sports floor material processing technology
环氧树脂运动地坪材料加工工艺
FANG XIA (Autor:in)
15.09.2023
Patent
Elektronische Ressource
Chinesisch
High-performance sports rubber floor and processing technology thereof
Europäisches Patentamt | 2022
|Waterproof anti-corrosion epoxy resin floor structure
Europäisches Patentamt | 2022
|