Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
The invention aims to provide the manufacturing method of the Lingnan cultural relic ancient building grey plastic prefabricated part, the method has higher preparation efficiency, and the grey plastic part manufactured by the method has better weather resistance. Comprising the following steps: S1, preparing grass gluten ash which contains prefabricated grass gluten and cement; s2, a skeleton of the component is manufactured, the skeleton is composed of a base and branch skeletons, and the metal wires serve as the branch skeletons; the metal wire is made into a spiral shape; s3, laying the grass gluten ash prepared in the step S1 on the framework in the step S2; s4, a weather-proof film layer is formed on the surface of the gray plastic part; s5, the grey plastic part which is just subjected to the step S4 is immediately subjected to coloring grey treatment; and S6, the grey plastic part is naturally air-dried and accumulated for more than 72 hours. The method has the advantages that the preparation time of the grass-gluten mortar is short, the grass-gluten mortar can be firmly bonded with grass-gluten mortar prepared by a traditional preparation method, the cracking degree is reduced, the grass-gluten mortar is not prone to being damaged and easy to repair, and the appearance and texture of a traditional grey plastic part are reserved.
本发明的目的在于提供一种岭南文物古建筑灰塑预制构件的制作方法,该方法具有较高的制备效率,且用该方法制得的灰塑件具有较好的耐候性。包括步骤S1:制备草筋灰,草筋灰中含有预制草筋和水泥;步骤S2:制作构件的骨架,骨架由基座和分支骨架组成,金属丝作为分支骨架;金属丝是被制成螺旋形的;步骤S3:将步骤S1所制备的草筋灰敷设到步骤S2的骨架上;步骤S4:令灰塑件表面形成耐候膜层;步骤S5:对刚实施了步骤S4的灰塑件马上进行上色灰处理;步骤S6:让灰塑件自然风干累积超过72小时。本发明具有草筋灰准备时间短、可与传统制法的草筋灰牢靠粘结、降低开裂程度、不易缺损、易于修复且保留传统灰塑件的外观和质感等优点。
The invention aims to provide the manufacturing method of the Lingnan cultural relic ancient building grey plastic prefabricated part, the method has higher preparation efficiency, and the grey plastic part manufactured by the method has better weather resistance. Comprising the following steps: S1, preparing grass gluten ash which contains prefabricated grass gluten and cement; s2, a skeleton of the component is manufactured, the skeleton is composed of a base and branch skeletons, and the metal wires serve as the branch skeletons; the metal wire is made into a spiral shape; s3, laying the grass gluten ash prepared in the step S1 on the framework in the step S2; s4, a weather-proof film layer is formed on the surface of the gray plastic part; s5, the grey plastic part which is just subjected to the step S4 is immediately subjected to coloring grey treatment; and S6, the grey plastic part is naturally air-dried and accumulated for more than 72 hours. The method has the advantages that the preparation time of the grass-gluten mortar is short, the grass-gluten mortar can be firmly bonded with grass-gluten mortar prepared by a traditional preparation method, the cracking degree is reduced, the grass-gluten mortar is not prone to being damaged and easy to repair, and the appearance and texture of a traditional grey plastic part are reserved.
本发明的目的在于提供一种岭南文物古建筑灰塑预制构件的制作方法,该方法具有较高的制备效率,且用该方法制得的灰塑件具有较好的耐候性。包括步骤S1:制备草筋灰,草筋灰中含有预制草筋和水泥;步骤S2:制作构件的骨架,骨架由基座和分支骨架组成,金属丝作为分支骨架;金属丝是被制成螺旋形的;步骤S3:将步骤S1所制备的草筋灰敷设到步骤S2的骨架上;步骤S4:令灰塑件表面形成耐候膜层;步骤S5:对刚实施了步骤S4的灰塑件马上进行上色灰处理;步骤S6:让灰塑件自然风干累积超过72小时。本发明具有草筋灰准备时间短、可与传统制法的草筋灰牢靠粘结、降低开裂程度、不易缺损、易于修复且保留传统灰塑件的外观和质感等优点。
Manufacturing method of Lingnan cultural relic ancient building grey sculpture prefabricated part
一种岭南文物古建筑灰塑预制构件的制作方法
LIU QIJUN (Autor:in)
10.11.2023
Patent
Elektronische Ressource
Chinesisch
Europäisches Patentamt | 2024
|Research on Conservation Planning Method of Lingnan Ancient Villages
British Library Conference Proceedings | 2011
|Analyses of Pathological Changes of Lingnan Ancient Stone Bridges
Trans Tech Publications | 2010
|Analyses of Pathological Changes of Lingnan Ancient Stone Bridges
British Library Conference Proceedings | 2011
|