Antiskid ceramic tile and preparation method thereof
The invention relates to an antiskid ceramic tile and a preparation method thereof, and belongs to the technical field of ceramics. The invention discloses a preparation method of an antiskid ceramic tile. The ceramic preparation process comprises the following steps: calcining a green body sprayed with cover glaze, coating with an etching liquid, coating with a paraffin antifouling layer, performing soft polishing, and coating with an antiskid layer. Etching liquid is used for etching the surface of the ceramic tile to increase the roughness and improve the antiskid performance; the paraffin antifouling layer permeates into small gaps and micro cracks on the surface layer of the ceramic tile to fill up the micro gaps in the ceramic tile, and physical and chemical reactions are generated in the ceramic tile, so that an anti-pollution protective film is generated; the anti-skid layer is formed by compositing wax liquid a and wax liquid b, a composite coating which is highly compact and high in transparency is formed after hardening, and certain roughness of the brick surface can be reserved through volume shrinkage after curing-hardening. The anti-slip ceramic tile which is anti-fouling, anti-slip and glossy can be prepared through the process.
本发明涉及一种防滑陶瓷砖及其制备方法,属于陶瓷技术领域。本发明公开了防滑陶瓷砖的制备方法,陶瓷制备的工艺步骤包括了已喷涂面釉的坯体进行煅烧—刻蚀液涂布—涂石蜡防污层—软抛光—涂防滑层。使用刻蚀液对陶瓷砖表面刻蚀增加粗糙度提高防滑性能;石蜡防污层渗入瓷砖表层的小缝隙和微裂缝中,填补瓷砖内部的微小空隙,在瓷砖内部产生物理和化学反应,从而产生抗污染保护膜;防滑层由蜡水a和蜡水b复合而成,硬化后形成一层高度致密、透明度高的复合涂层,固化-硬化后体积收缩可以使砖面保留一定的粗糙度。本发明通过以上工艺可制备出防污、防滑并具有光泽的防滑陶瓷砖。
Antiskid ceramic tile and preparation method thereof
The invention relates to an antiskid ceramic tile and a preparation method thereof, and belongs to the technical field of ceramics. The invention discloses a preparation method of an antiskid ceramic tile. The ceramic preparation process comprises the following steps: calcining a green body sprayed with cover glaze, coating with an etching liquid, coating with a paraffin antifouling layer, performing soft polishing, and coating with an antiskid layer. Etching liquid is used for etching the surface of the ceramic tile to increase the roughness and improve the antiskid performance; the paraffin antifouling layer permeates into small gaps and micro cracks on the surface layer of the ceramic tile to fill up the micro gaps in the ceramic tile, and physical and chemical reactions are generated in the ceramic tile, so that an anti-pollution protective film is generated; the anti-skid layer is formed by compositing wax liquid a and wax liquid b, a composite coating which is highly compact and high in transparency is formed after hardening, and certain roughness of the brick surface can be reserved through volume shrinkage after curing-hardening. The anti-slip ceramic tile which is anti-fouling, anti-slip and glossy can be prepared through the process.
本发明涉及一种防滑陶瓷砖及其制备方法,属于陶瓷技术领域。本发明公开了防滑陶瓷砖的制备方法,陶瓷制备的工艺步骤包括了已喷涂面釉的坯体进行煅烧—刻蚀液涂布—涂石蜡防污层—软抛光—涂防滑层。使用刻蚀液对陶瓷砖表面刻蚀增加粗糙度提高防滑性能;石蜡防污层渗入瓷砖表层的小缝隙和微裂缝中,填补瓷砖内部的微小空隙,在瓷砖内部产生物理和化学反应,从而产生抗污染保护膜;防滑层由蜡水a和蜡水b复合而成,硬化后形成一层高度致密、透明度高的复合涂层,固化-硬化后体积收缩可以使砖面保留一定的粗糙度。本发明通过以上工艺可制备出防污、防滑并具有光泽的防滑陶瓷砖。
Antiskid ceramic tile and preparation method thereof
一种防滑陶瓷砖及其制备方法
SUN HUAXIN (Autor:in) / WANG JIANXIAN (Autor:in) / ZHU QINFANG (Autor:in) / YUAN DINGYAN (Autor:in)
02.02.2024
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Antiskid ceramic tile and preparation process thereof
Europäisches Patentamt | 2024
|Antiskid ceramic floor tile and preparation method thereof
Europäisches Patentamt | 2024
|Antiskid wear-resistant ceramic tile and preparation method thereof
Europäisches Patentamt | 2023
|Super-antiskid multifunctional ceramic tile and preparation method thereof
Europäisches Patentamt | 2024
|