Coal-saving and consumption-reducing cement mineralizer and preparation method thereof
The invention relates to the technical field of cement manufacturing, in particular to a coal-saving and consumption-reducing cement mineralizer and a preparation method thereof.The cement mineralizer is prepared from, by weight, 10-15 parts of polyhydric alcohol amine, 5-10 parts of calcium fluoride, 5-10 parts of organic acid salt, 8-15 parts of acryloyloxy ammonium salt, 8-15 parts of tartaric acid, 5-10 parts of molasses, 5 parts of nano calcium silicate hydrate, 5-10 parts of treating agent and 20-54 parts of water. Through reasonable formula design and product compounding, the special cement mineralizing agent which is free of chlorine, alkali and pollution and is green and environment-friendly is prepared by utilizing the synergistic effect of all the substances.
本发明涉及水泥制造技术领域,特别涉及一种节煤降耗的水泥矿化剂及其制备方法,所述水泥矿化剂按重量份计,包括如下组分:多元醇胺10~15份,氟化钙5~10份,有机酸盐5~10份,丙烯酰氧铵盐8~15份,酒石酸8~15份,糖蜜5~10份,纳米水化硅酸钙5份,处理剂5~10份和水20~54份。本发明通过合理的配方设计和产品复配,利用各物质之间的协同配合作用,制造出无氯无碱、绿色环保、无污染的专用水泥矿化剂。
Coal-saving and consumption-reducing cement mineralizer and preparation method thereof
The invention relates to the technical field of cement manufacturing, in particular to a coal-saving and consumption-reducing cement mineralizer and a preparation method thereof.The cement mineralizer is prepared from, by weight, 10-15 parts of polyhydric alcohol amine, 5-10 parts of calcium fluoride, 5-10 parts of organic acid salt, 8-15 parts of acryloyloxy ammonium salt, 8-15 parts of tartaric acid, 5-10 parts of molasses, 5 parts of nano calcium silicate hydrate, 5-10 parts of treating agent and 20-54 parts of water. Through reasonable formula design and product compounding, the special cement mineralizing agent which is free of chlorine, alkali and pollution and is green and environment-friendly is prepared by utilizing the synergistic effect of all the substances.
本发明涉及水泥制造技术领域,特别涉及一种节煤降耗的水泥矿化剂及其制备方法,所述水泥矿化剂按重量份计,包括如下组分:多元醇胺10~15份,氟化钙5~10份,有机酸盐5~10份,丙烯酰氧铵盐8~15份,酒石酸8~15份,糖蜜5~10份,纳米水化硅酸钙5份,处理剂5~10份和水20~54份。本发明通过合理的配方设计和产品复配,利用各物质之间的协同配合作用,制造出无氯无碱、绿色环保、无污染的专用水泥矿化剂。
Coal-saving and consumption-reducing cement mineralizer and preparation method thereof
一种节煤降耗的水泥矿化剂及其制备方法
HUANG HUANG (Autor:in) / CHEN WEI (Autor:in) / LIAO WENJIE (Autor:in) / LONG CAIXIA (Autor:in) / LIANG HUI (Autor:in) / YIN DAN (Autor:in) / WANG HENG (Autor:in)
01.03.2024
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
NOVEL FLUX / MINERALIZER FOR CEMENT CLINKERING AND METHOD OF MANUFACTURE THEREOF
Europäisches Patentamt | 2021
|Novel energy-saving consumption-reducing dry-process cement clinker and preparation method thereof
Europäisches Patentamt | 2015
|Optimal fluorite/gypsum mineralizer ratio in Portland cement clinkering
DOAJ | 2016
|