Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Method for improving expansibility of soil and sludge mixed ceramsite
The invention discloses a method for improving the expansibility of soil and sludge mixed ceramsite, and relates to the technical field of expanded ceramsite, the method for improving the expansibility of the soil and sludge mixed ceramsite comprises the following operation steps: S1, screening and detecting raw materials; s2, performing normalization processing; s3, preparing green pellets; s4, measuring the sintering temperature of the ceramsite; and S5, determining the expansion condition of the ceramsite. According to the method for improving the expansibility of the soil and sludge mixed ceramsite, the firing process of the ceramsite is changed, auxiliary materials are added, the firing effect of the ceramsite is improved, the economic input is reduced, the economic income is increased, the problem that various properties of the fired ceramsite are not greatly improved is solved, auxiliary materials do not need to be added, and energy consumption is reduced; compared with a common firing method, the fired ceramsite is expanded by at least two times in volume, the requirement for raw material components is lowered, the firing temperature is lower than the conventional firing temperature, control is easy, and energy consumption is reduced.
本发明公开了一种提高土壤、污泥混合陶粒膨胀性的方法,涉及膨胀陶粒技术领域,所述提高土壤、污泥混合陶粒膨胀性的方法包括下述操作步骤:S1、原料过筛和检测;S2、归一处理;S3、制备生粒球;S4、测定陶粒的烧熔温度;S5、测定陶粒的膨胀条件。该提高土壤、污泥混合陶粒膨胀性的方法,通过改变陶粒的烧制工艺解决添加辅料改善陶粒烧制效果,降低了经济投入,增加了经济收入,解决了烧出来的陶粒各方面性能改善不大的难题,无需添加辅料且节约能耗,烧制出的陶粒较普通烧制方法至少膨胀两倍体积,对原料成分要求有所降低,且烧制温度较常规烧制温度低,易于控制且减少能耗。
Method for improving expansibility of soil and sludge mixed ceramsite
The invention discloses a method for improving the expansibility of soil and sludge mixed ceramsite, and relates to the technical field of expanded ceramsite, the method for improving the expansibility of the soil and sludge mixed ceramsite comprises the following operation steps: S1, screening and detecting raw materials; s2, performing normalization processing; s3, preparing green pellets; s4, measuring the sintering temperature of the ceramsite; and S5, determining the expansion condition of the ceramsite. According to the method for improving the expansibility of the soil and sludge mixed ceramsite, the firing process of the ceramsite is changed, auxiliary materials are added, the firing effect of the ceramsite is improved, the economic input is reduced, the economic income is increased, the problem that various properties of the fired ceramsite are not greatly improved is solved, auxiliary materials do not need to be added, and energy consumption is reduced; compared with a common firing method, the fired ceramsite is expanded by at least two times in volume, the requirement for raw material components is lowered, the firing temperature is lower than the conventional firing temperature, control is easy, and energy consumption is reduced.
本发明公开了一种提高土壤、污泥混合陶粒膨胀性的方法,涉及膨胀陶粒技术领域,所述提高土壤、污泥混合陶粒膨胀性的方法包括下述操作步骤:S1、原料过筛和检测;S2、归一处理;S3、制备生粒球;S4、测定陶粒的烧熔温度;S5、测定陶粒的膨胀条件。该提高土壤、污泥混合陶粒膨胀性的方法,通过改变陶粒的烧制工艺解决添加辅料改善陶粒烧制效果,降低了经济投入,增加了经济收入,解决了烧出来的陶粒各方面性能改善不大的难题,无需添加辅料且节约能耗,烧制出的陶粒较普通烧制方法至少膨胀两倍体积,对原料成分要求有所降低,且烧制温度较常规烧制温度低,易于控制且减少能耗。
Method for improving expansibility of soil and sludge mixed ceramsite
一种提高土壤、污泥混合陶粒膨胀性的方法
LIU RENHUA (Autor:in) / ZHU KAIZHEN (Autor:in) / SUN JIASHAN (Autor:in) / WEN YURONG (Autor:in) / JIA XINGLIANG (Autor:in)
01.03.2024
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Method for preparing ceramsite by recycling polluted soil and boric sludge and ceramsite
Europäisches Patentamt | 2023
|Ceramsite cooling device for sludge ceramsite preparation
Europäisches Patentamt | 2020
|