Shale hollow brick and thermal insulation wall construction method using shale hollow brick
The invention discloses a shale hollow brick which is characterized by comprising the following components in parts by weight: 65-70 parts of shale, 10-15 parts of industrial waste soil, 5-10 parts of thermal insulation particles, 1-5 parts of binder, 10-20 parts of pore-forming agent and 10-15 parts of water. The shale hollow brick is prepared from the following components in parts by weight: 65-70 parts of shale, 10-15 parts of industrial waste soil, 5-10 parts of thermal insulation particles, 1-5 parts of binder, 10-20 parts of pore-forming agent and 10-15 parts of water. Compared with the prior art, the shale hollow brick and the construction method of the thermal insulation wall using the shale hollow brick have the advantages that the shale hollow brick is convenient to use, stable in performance and good in strength and can be conveniently used as the thermal insulation wall.
本发明公开了一种页岩空心砖,其特征在于:包括页岩、工业废土、保温颗粒、粘结剂、成孔剂和水,其中各个组分比为页岩65~70份、工业废土10~15份、保温颗粒5~10、粘结剂1~5份、成孔剂10~20份和水10~15份的水。本发明与现有技术相比的优点在于:提供一种方便使用,性能稳定,强度好,方便作为保温墙体使用的一种页岩空心砖及使用页岩空心砖的保温墙体施工方法。
Shale hollow brick and thermal insulation wall construction method using shale hollow brick
The invention discloses a shale hollow brick which is characterized by comprising the following components in parts by weight: 65-70 parts of shale, 10-15 parts of industrial waste soil, 5-10 parts of thermal insulation particles, 1-5 parts of binder, 10-20 parts of pore-forming agent and 10-15 parts of water. The shale hollow brick is prepared from the following components in parts by weight: 65-70 parts of shale, 10-15 parts of industrial waste soil, 5-10 parts of thermal insulation particles, 1-5 parts of binder, 10-20 parts of pore-forming agent and 10-15 parts of water. Compared with the prior art, the shale hollow brick and the construction method of the thermal insulation wall using the shale hollow brick have the advantages that the shale hollow brick is convenient to use, stable in performance and good in strength and can be conveniently used as the thermal insulation wall.
本发明公开了一种页岩空心砖,其特征在于:包括页岩、工业废土、保温颗粒、粘结剂、成孔剂和水,其中各个组分比为页岩65~70份、工业废土10~15份、保温颗粒5~10、粘结剂1~5份、成孔剂10~20份和水10~15份的水。本发明与现有技术相比的优点在于:提供一种方便使用,性能稳定,强度好,方便作为保温墙体使用的一种页岩空心砖及使用页岩空心砖的保温墙体施工方法。
Shale hollow brick and thermal insulation wall construction method using shale hollow brick
一种页岩空心砖及使用页岩空心砖的保温墙体施工方法
ZHANG DAN (Autor:in) / WU BIN (Autor:in) / JIANG BO (Autor:in) / ZHANG XINGXING (Autor:in) / PANG ERJUN (Autor:in)
07.06.2024
Patent
Elektronische Ressource
Chinesisch
Coal gangue shale flyash insulation hollow brick and preparation method thereof
Europäisches Patentamt | 2015
|