Early hardening concrete and production method thereof
The invention relates to the technical field of early hardening concrete, in particular to early hardening concrete and a production method thereof.The concrete is prepared from, by mass, 60-80 parts of cement, 80-100 parts of aggregate, 60-80 parts of filler, 10-15 parts of admixture and 70-90 parts of water, and the production method comprises the following steps of material preparing, material mixing operation, admixture adding, outputting and transferring. According to the invention, by adding the corresponding admixture, filler and the like into the cement and the aggregate, the setting quality of the concrete is fully improved, the time required for setting is shortened, and the hardness during early-stage setting is fully ensured, so that the corresponding operation is conveniently carried out; meanwhile, it can be effectively and fully guaranteed that heat is taken away, the situation that the concrete bursts after being coagulated is avoided, meanwhile, the production and preparation mode of the early hardening concrete shows that preparation by workers is facilitated, and the preparation quality of the concrete is guaranteed.
本发明涉及早硬性混凝土技术领域,具体为一种早硬性混凝土及其生产方法,其混凝土按质量份数计,包括以下组分:水泥60‑80、骨料80‑100、填充料60‑80、外加剂10‑15、水70‑90,其生产方法包括以下步骤:备料、混料作业、外加剂添加和输出转运。本发明本申请通过向水泥和骨料中添加相应的外加剂和填充料等在充分提升混凝土凝结质量的同时缩短其凝结所需时间,并且充分保证早期凝结时的硬度,以便进行相应的操作,同时还能有效充分保证带走热量避免混凝土凝结后出现爆裂的情况,同时还针对本早硬性混凝土的生产制备的方式进行表明,便于工作人员进行制备,保证混凝土的制备质量。
Early hardening concrete and production method thereof
The invention relates to the technical field of early hardening concrete, in particular to early hardening concrete and a production method thereof.The concrete is prepared from, by mass, 60-80 parts of cement, 80-100 parts of aggregate, 60-80 parts of filler, 10-15 parts of admixture and 70-90 parts of water, and the production method comprises the following steps of material preparing, material mixing operation, admixture adding, outputting and transferring. According to the invention, by adding the corresponding admixture, filler and the like into the cement and the aggregate, the setting quality of the concrete is fully improved, the time required for setting is shortened, and the hardness during early-stage setting is fully ensured, so that the corresponding operation is conveniently carried out; meanwhile, it can be effectively and fully guaranteed that heat is taken away, the situation that the concrete bursts after being coagulated is avoided, meanwhile, the production and preparation mode of the early hardening concrete shows that preparation by workers is facilitated, and the preparation quality of the concrete is guaranteed.
本发明涉及早硬性混凝土技术领域,具体为一种早硬性混凝土及其生产方法,其混凝土按质量份数计,包括以下组分:水泥60‑80、骨料80‑100、填充料60‑80、外加剂10‑15、水70‑90,其生产方法包括以下步骤:备料、混料作业、外加剂添加和输出转运。本发明本申请通过向水泥和骨料中添加相应的外加剂和填充料等在充分提升混凝土凝结质量的同时缩短其凝结所需时间,并且充分保证早期凝结时的硬度,以便进行相应的操作,同时还能有效充分保证带走热量避免混凝土凝结后出现爆裂的情况,同时还针对本早硬性混凝土的生产制备的方式进行表明,便于工作人员进行制备,保证混凝土的制备质量。
Early hardening concrete and production method thereof
一种早硬性混凝土及其生产方法
YANG YADONG (Autor:in) / MA HULIN (Autor:in) / WANG ZHENYANG (Autor:in) / SHI HAITAO (Autor:in) / YANG HONGXIA (Autor:in) / MA ZHAOPING (Autor:in) / WANG ANRU (Autor:in) / XU LE (Autor:in) / LI QIANG (Autor:in) / LI WEI (Autor:in)
08.11.2024
Patent
Elektronische Ressource
Chinesisch
QUICK-HARDENING CONCRETE AND PRODUCTION METHOD THEREOF
Europäisches Patentamt | 2015
|RAPID HARDENING CONCRETE AND PRODUCTION METHOD THEREOF
Europäisches Patentamt | 2018
|Early-strength rapid-hardening conductive concrete and preparation method thereof
Europäisches Patentamt | 2024
|Quick-hardening early-strength sulphoaluminate cement concrete and preparation method thereof
Europäisches Patentamt | 2023
|Europäisches Patentamt | 2024
|