Reinforcing method and reinforcing device for quickly reinforcing bone keratin cultural relics
The invention relates to the technical field of cultural relic reinforcing, in particular to a reinforcing method and a reinforcing device for quickly reinforcing bone keratin cultural relics, which are particularly suitable for reinforcing the bone keratin cultural relics in archaeological sites. A reinforcing method for rapidly reinforcing bone keratin cultural relics comprises the following steps that nano calcium hydroxide suspension liquid is introduced into the unearthed and waterlogged bone keratin cultural relics, and the bone keratin cultural relics are placed in a closed environment; preparing a supersaturated salt solution, and placing the supersaturated salt solution in a closed environment; introducing carbon dioxide into the closed environment; and detecting calcium hydroxide introduced into the bone keratin cultural relics by using a Raman spectrometer, and reinforcing the bone keratin cultural relics when no calcium hydroxide is detected. And the bone keratin cultural relics are reinforced.
本申请涉及文物加固技术领域,具体涉及一种用于骨角质文物快速加固的加固方法和加固装置,尤其适合用于考古现场的骨角质文物的加固。一种用于骨角质文物快速加固的加固方法,所述方法包括如下步骤:向出土饱水的骨角质文物引入纳米氢氧化钙悬浮液,将所述骨角质文物放置到密闭环境中;配置过饱和盐溶液,将所述过饱和盐溶液放置到密闭环境中;向所述密闭环境中通入二氧化碳;利用拉曼光谱仪检测引入骨角质文物中的氢氧化钙,当未检测到氢氧化钙时完成对所述骨角质文物的加固。实现对于骨角质文物的加固。
Reinforcing method and reinforcing device for quickly reinforcing bone keratin cultural relics
The invention relates to the technical field of cultural relic reinforcing, in particular to a reinforcing method and a reinforcing device for quickly reinforcing bone keratin cultural relics, which are particularly suitable for reinforcing the bone keratin cultural relics in archaeological sites. A reinforcing method for rapidly reinforcing bone keratin cultural relics comprises the following steps that nano calcium hydroxide suspension liquid is introduced into the unearthed and waterlogged bone keratin cultural relics, and the bone keratin cultural relics are placed in a closed environment; preparing a supersaturated salt solution, and placing the supersaturated salt solution in a closed environment; introducing carbon dioxide into the closed environment; and detecting calcium hydroxide introduced into the bone keratin cultural relics by using a Raman spectrometer, and reinforcing the bone keratin cultural relics when no calcium hydroxide is detected. And the bone keratin cultural relics are reinforced.
本申请涉及文物加固技术领域,具体涉及一种用于骨角质文物快速加固的加固方法和加固装置,尤其适合用于考古现场的骨角质文物的加固。一种用于骨角质文物快速加固的加固方法,所述方法包括如下步骤:向出土饱水的骨角质文物引入纳米氢氧化钙悬浮液,将所述骨角质文物放置到密闭环境中;配置过饱和盐溶液,将所述过饱和盐溶液放置到密闭环境中;向所述密闭环境中通入二氧化碳;利用拉曼光谱仪检测引入骨角质文物中的氢氧化钙,当未检测到氢氧化钙时完成对所述骨角质文物的加固。实现对于骨角质文物的加固。
Reinforcing method and reinforcing device for quickly reinforcing bone keratin cultural relics
一种用于骨角质文物快速加固的加固方法和加固装置
MA XIAO (Autor:in) / NIU MENGHAO (Autor:in) / WANG PENGJIE (Autor:in)
10.12.2024
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Auxiliary device for reinforcing building cultural relics
Europäisches Patentamt | 2024
|Device and method for reinforcing rock cultural relics
Europäisches Patentamt | 2024
|Europäisches Patentamt | 2015
|Method for reinforcing silicate cultural relics through hyperbranched polysiloxane and application
Europäisches Patentamt | 2021
|Building cultural relic reinforcing device and reinforcing method thereof
Europäisches Patentamt | 2024
|