Hydrophilic self-cleaning glaze, hydrophilic self-cleaning archaized brick and preparation method of hydrophilic self-cleaning archaized brick
The invention discloses a hydrophilic self-cleaning glaze which comprises the following components in percentage by mass: 75-95% of hydrophilic frit and 5-25% of kaolin, the hydrophilic frit comprises the following components in percentage by mass: 2-4% of boric acid, 5-9% of lithium carbonate, 30-40% of wollastonite, 9-16% of calcined talc, 10-20% of kaolin, 13-22% of quartz and 8-12% of aluminum oxide. According to the hydrophilic self-cleaning glaze provided by the invention, on the premise of reducing the production cost, excellent and lasting self-cleaning performance can be realized, and the technical problem of poor timeliness of self-cleaning performance in the prior art is solved.
本发明公开了一种亲水自洁釉料,按照质量百分比计算,包括亲水熔块75~95%和高岭土5~25%;按照质量百分比计算,所述亲水熔块包括硼酸2~4%、碳酸锂5~9%、硅灰石30~40%、烧滑石9~16%、高岭土10~20%、石英13~22%和氧化铝8~12%。本发明提出的一种亲水自洁釉料,在降低生产成本的前提下,能实现优异且持久的自洁性,解决了现有技术中自洁性时效性差的技术问题。
Hydrophilic self-cleaning glaze, hydrophilic self-cleaning archaized brick and preparation method of hydrophilic self-cleaning archaized brick
The invention discloses a hydrophilic self-cleaning glaze which comprises the following components in percentage by mass: 75-95% of hydrophilic frit and 5-25% of kaolin, the hydrophilic frit comprises the following components in percentage by mass: 2-4% of boric acid, 5-9% of lithium carbonate, 30-40% of wollastonite, 9-16% of calcined talc, 10-20% of kaolin, 13-22% of quartz and 8-12% of aluminum oxide. According to the hydrophilic self-cleaning glaze provided by the invention, on the premise of reducing the production cost, excellent and lasting self-cleaning performance can be realized, and the technical problem of poor timeliness of self-cleaning performance in the prior art is solved.
本发明公开了一种亲水自洁釉料,按照质量百分比计算,包括亲水熔块75~95%和高岭土5~25%;按照质量百分比计算,所述亲水熔块包括硼酸2~4%、碳酸锂5~9%、硅灰石30~40%、烧滑石9~16%、高岭土10~20%、石英13~22%和氧化铝8~12%。本发明提出的一种亲水自洁釉料,在降低生产成本的前提下,能实现优异且持久的自洁性,解决了现有技术中自洁性时效性差的技术问题。
Hydrophilic self-cleaning glaze, hydrophilic self-cleaning archaized brick and preparation method of hydrophilic self-cleaning archaized brick
一种亲水自洁釉料、亲水自洁仿古砖及其制备方法
LI SUBO (Autor:in) / LI ZHIHONG (Autor:in) / XU YU (Autor:in) / ZHONG BAOMIN (Autor:in) / LUO QIANG (Autor:in) / XIE SUI (Autor:in)
17.12.2024
Patent
Elektronische Ressource
Chinesisch
Hydrophilic self-cleaning archaized brick and preparation method thereof
Europäisches Patentamt | 2024
|Method for preparing archaized brick with wear-resistant glaze and archaized brick
Europäisches Patentamt | 2023
|Glaze for low-radioactivity archaized brick, brick applying glaze and preparation method
Europäisches Patentamt | 2023
|Archaized brick prepared from waste ceramic and preparation method of archaized brick
Europäisches Patentamt | 2023
|Archaized brick framework and archaized brick pressing production method
Europäisches Patentamt | 2021
|