The invention relates to an autoclaved aerated concrete self-heat-preservation building block and a preparation method thereof, and belongs to the technical field of new building materials, the autoclaved aerated concrete self-heat-preservation building block comprises aggregate and water, and the water-material ratio is 0.4-0.6; the aggregate is prepared from the following components in parts by mass: 50 to 80 parts of fly ash or quartz sand, 4 to 20 parts of cement, 5 to 20 parts of quick lime, 0 to 5 parts of gypsum, 0.05 to 0.15 part of aluminum paste and 2 to 3 parts of a special additive for self-insulation. The invention also discloses a preparation method of the autoclaved aerated concrete self-insulation building block. The autoclaved aerated concrete self-insulation building block has the advantages of high strength and low heat conductivity.
本发明涉及一种蒸压加气混凝土自保温砌块及其制备方法,属于建筑新材料的技术领域,包括骨料和水,水料比为0.4~0.6;所述骨料按质量份数计,包括粉煤灰或石英砂50~80份、水泥4~20份、生石灰5~20份、石膏0~5份、铝膏0.05~0.15份和自保温专用外加剂2~3份。本发明还公开了蒸压加气混凝土自保温砌块的制备方法。本发明蒸压加气混凝土自保温砌块具有高强度、低导热的优势。
The invention relates to an autoclaved aerated concrete self-heat-preservation building block and a preparation method thereof, and belongs to the technical field of new building materials, the autoclaved aerated concrete self-heat-preservation building block comprises aggregate and water, and the water-material ratio is 0.4-0.6; the aggregate is prepared from the following components in parts by mass: 50 to 80 parts of fly ash or quartz sand, 4 to 20 parts of cement, 5 to 20 parts of quick lime, 0 to 5 parts of gypsum, 0.05 to 0.15 part of aluminum paste and 2 to 3 parts of a special additive for self-insulation. The invention also discloses a preparation method of the autoclaved aerated concrete self-insulation building block. The autoclaved aerated concrete self-insulation building block has the advantages of high strength and low heat conductivity.
本发明涉及一种蒸压加气混凝土自保温砌块及其制备方法,属于建筑新材料的技术领域,包括骨料和水,水料比为0.4~0.6;所述骨料按质量份数计,包括粉煤灰或石英砂50~80份、水泥4~20份、生石灰5~20份、石膏0~5份、铝膏0.05~0.15份和自保温专用外加剂2~3份。本发明还公开了蒸压加气混凝土自保温砌块的制备方法。本发明蒸压加气混凝土自保温砌块具有高强度、低导热的优势。
Autoclaved aerated concrete self-insulation building block and preparation method thereof
一种蒸压加气混凝土自保温砌块及其制备方法
LYU HAIBO (Autor:in)
24.12.2024
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Autoclaved aerated concrete self-insulation building block and manufacturing process thereof
Europäisches Patentamt | 2024
|Europäisches Patentamt | 2022
|Preparation method of autoclaved aerated concrete block and autoclaved aerated concrete block
Europäisches Patentamt | 2021
|Autoclaved aerated concrete building block and preparation method thereof
Europäisches Patentamt | 2015
|Europäisches Patentamt | 2016
|