LAYERED INTERFACE COATING FOR IMPROVED FIBER PROTECTION AND MATRIX CRACK SEALING
A coated fiber structure for use in a ceramic matrix composite comprises a fiber extending along a fiber axis and an interface coating arrangement applied to and circumscribing the fiber. The interface coating arrangement comprises: a first boron nitride layer extending coaxially about and in direct contact with the fiber, a first silicon-doped boron nitride layer extending coaxially about and in direct contact with the first boron nitride layer, a carbon layer extending coaxially about and in direct contact with the first silicon-doped boron nitride layer, a second boron nitride layer extending coaxially about and in direct contact with the carbon layer, and a second silicon-doped boron nitride layer extending coaxially about and in direct contact with the second boron nitride layer. A silicon content of the first silicon-doped boron nitride layer is higher than the silicon content of the second silicon-doped boron nitride layer.
LAYERED INTERFACE COATING FOR IMPROVED FIBER PROTECTION AND MATRIX CRACK SEALING
A coated fiber structure for use in a ceramic matrix composite comprises a fiber extending along a fiber axis and an interface coating arrangement applied to and circumscribing the fiber. The interface coating arrangement comprises: a first boron nitride layer extending coaxially about and in direct contact with the fiber, a first silicon-doped boron nitride layer extending coaxially about and in direct contact with the first boron nitride layer, a carbon layer extending coaxially about and in direct contact with the first silicon-doped boron nitride layer, a second boron nitride layer extending coaxially about and in direct contact with the carbon layer, and a second silicon-doped boron nitride layer extending coaxially about and in direct contact with the second boron nitride layer. A silicon content of the first silicon-doped boron nitride layer is higher than the silicon content of the second silicon-doped boron nitride layer.
LAYERED INTERFACE COATING FOR IMPROVED FIBER PROTECTION AND MATRIX CRACK SEALING
GESCHICHTETE SCHNITTSTELLENBESCHICHTUNG FÜR VERBESSERTEN FASERSCHUTZ UND VERBESSERTE MATRIXRISSDICHTUNG
REVÊTEMENT D'INTERFACE STRATIFIÉ POUR UNE PROTECTION DE FIBRE AMÉLIORÉE ET UNE ÉTANCHÉITÉ DE FISSURE DE MATRICE AMÉLIORÉE
CALLAWAY EVAN B (Autor:in)
25.12.2024
Patent
Elektronische Ressource
Englisch
IPC:
C04B
Kalk
,
LIME
LAYERED INTERFACE COATING FOR IMPROVED FIBER PROTECTION AND MATRIX CRACK SEALING
Europäisches Patentamt | 2024
|LAYERED INTERFACE COATING FOR IMPROVED FIBER PROTECTION AND MATRIX CRACK SEALING
Europäisches Patentamt | 2024
|Interface crack in periodically layered bimaterial composite
British Library Online Contents | 2002
|Layered silicates nanocomposite matrix for improved fiber reinforced composites properties
British Library Online Contents | 2009
|The fiber-matrix interface crack - A numerical analysis using Boundary Elements
British Library Online Contents | 1996
|