PLASTIC INJECTION MATERIAL, AND PRODUCTION METHOD THEREOF
PROBLEM TO BE SOLVED: To provide a plastic injection material in which liquid A and liquid B are prevented from being hardened individually so that flowability of each of the liquid A and the liquid B can be kept in an extent that each of them can be sent forcibly and the amount of the hydrated lime to be blended can be reduced, and to provide a production method of the plastic injection material.SOLUTION: The liquid A containing blast furnace slag, bentonite, and water is mixed with the liquid B containing hydrated lime and water to form the plastic injection material. Aluminate of 3-12 pts. mass on the basis of 100 pts. mass of the bentonite is further incorporated in the liquid A. The amount of the hydrated lime in the liquid B is adjusted to 5-20 pts. mass on the basis of 100 pts. mass of the blast furnace slag in the liquid A.
【課題】A液およびB液が個別に硬化するのを防止することでA液およびB液の流動性を圧送可能な程度に維持することができると共に、消石灰の配合量を低減することができる可塑性注入材およびその製造方法を提供することを課題とする。【解決手段】高炉スラグとベントナイトと水とを含有するA液と、消石灰と水とを含有するB液とが混合されて形成される可塑性注入材であって、B液は、A液中のベントナイト100質量部に対して3質量部以上12質量部以下のアルミン酸塩を更に含有すると共に、A液中の高炉スラグ100質量部に対して消石灰が5質量部以上20質量部以下となるように構成されることを特徴とする。【選択図】なし
PLASTIC INJECTION MATERIAL, AND PRODUCTION METHOD THEREOF
PROBLEM TO BE SOLVED: To provide a plastic injection material in which liquid A and liquid B are prevented from being hardened individually so that flowability of each of the liquid A and the liquid B can be kept in an extent that each of them can be sent forcibly and the amount of the hydrated lime to be blended can be reduced, and to provide a production method of the plastic injection material.SOLUTION: The liquid A containing blast furnace slag, bentonite, and water is mixed with the liquid B containing hydrated lime and water to form the plastic injection material. Aluminate of 3-12 pts. mass on the basis of 100 pts. mass of the bentonite is further incorporated in the liquid A. The amount of the hydrated lime in the liquid B is adjusted to 5-20 pts. mass on the basis of 100 pts. mass of the blast furnace slag in the liquid A.
【課題】A液およびB液が個別に硬化するのを防止することでA液およびB液の流動性を圧送可能な程度に維持することができると共に、消石灰の配合量を低減することができる可塑性注入材およびその製造方法を提供することを課題とする。【解決手段】高炉スラグとベントナイトと水とを含有するA液と、消石灰と水とを含有するB液とが混合されて形成される可塑性注入材であって、B液は、A液中のベントナイト100質量部に対して3質量部以上12質量部以下のアルミン酸塩を更に含有すると共に、A液中の高炉スラグ100質量部に対して消石灰が5質量部以上20質量部以下となるように構成されることを特徴とする。【選択図】なし
PLASTIC INJECTION MATERIAL, AND PRODUCTION METHOD THEREOF
可塑性注入材および可塑性注入材の製造方法
SATO TAKANOBU (Autor:in) / ARAKI ICHIJI (Autor:in)
16.07.2015
Patent
Elektronische Ressource
Japanisch
PLASTIC INJECTION MATERIAL, PRODUCTION METHOD THEREOF, AND EXECUTION METHOD THEREOF
Europäisches Patentamt | 2018
|PLASTIC INJECTION MATERIAL, PRODUCTION METHOD THEREOF, AND EXECUTION METHOD THEREOF
Europäisches Patentamt | 2016
|PLASTIC INJECTION MATERIAL, PRODUCTION METHOD THEREOF, AND EXECUTION METHOD THEREOF
Europäisches Patentamt | 2016
|Europäisches Patentamt | 2015
|Europäisches Patentamt | 2022
|