MANUFACTURING METHOD OF LOW FLUID MIXTURE
PROBLEM TO BE SOLVED: To provide a method capable of reducing fluidity of a solid-liquid mixture, while restraining a volume increase in a short time by simple work, regardless of a chemical composition of the solid-liquid mixture.SOLUTION: The prevent invention is a manufacturing method of a low fluid mixture including acquiring the low fluid mixture by mixing a solid-liquid mixture and a fluidity reduction agent of the solid-liquid mixture in a container. The fluidity reduction agent includes a granular material having a structure of entangling fiber, and the granular material is 300 μm or less in an average particle diameter, and is 0.25 m/g-100 m/g in the specific surface area by a BET method, or is 50% or more in the void ratio calculated by (1-bulk density/true density)×100, and is 0.25 m/g-100 m/g in the specific surface area by the BET method. The solid-liquid mixture is mixed in a quantity of 50 volume%-100 volume% to the mounting target volume of the low fluid mixture to the container, and the sum total of the use volume of the solid-liquid mixture and the fluidity reduction agent exceeds the mounting target volume of the low fluidity mixture to the container.SELECTED DRAWING: Figure 1
【課題】固液混合物の化学的組成によらず、短時間で簡易な作業により、容積増加を抑制しつつ、固液混合物の流動性を低下させることができる方法を提供する。【解決手段】本発明は、固液混合物と、前記固液混合物の流動性低下剤とを容器内で混合して低流動性混合物を得ることを含む、低流動性混合物の製造方法である。流動性低下剤は、繊維が絡み合った構造を有する粒状物を含み、粒状物は、平均粒子径が300μm以下かつBET法による比表面積が0.25m2/g以上100m2/g以下であり、又は(1−かさ密度/真密度)×100で計算される空隙率が50%以上かつBET法による比表面積が0.25m2/g以上100m2/g以下である。容器への低流動性混合物の搭載目標容積に対して、固液混合物が50容積%以上100容積%未満の量で混合され、かつ固液混合物及び流動性低下剤の使用容積の合計が容器への低流動性混合物の搭載目標容積を超える。【選択図】図1
MANUFACTURING METHOD OF LOW FLUID MIXTURE
PROBLEM TO BE SOLVED: To provide a method capable of reducing fluidity of a solid-liquid mixture, while restraining a volume increase in a short time by simple work, regardless of a chemical composition of the solid-liquid mixture.SOLUTION: The prevent invention is a manufacturing method of a low fluid mixture including acquiring the low fluid mixture by mixing a solid-liquid mixture and a fluidity reduction agent of the solid-liquid mixture in a container. The fluidity reduction agent includes a granular material having a structure of entangling fiber, and the granular material is 300 μm or less in an average particle diameter, and is 0.25 m/g-100 m/g in the specific surface area by a BET method, or is 50% or more in the void ratio calculated by (1-bulk density/true density)×100, and is 0.25 m/g-100 m/g in the specific surface area by the BET method. The solid-liquid mixture is mixed in a quantity of 50 volume%-100 volume% to the mounting target volume of the low fluid mixture to the container, and the sum total of the use volume of the solid-liquid mixture and the fluidity reduction agent exceeds the mounting target volume of the low fluidity mixture to the container.SELECTED DRAWING: Figure 1
【課題】固液混合物の化学的組成によらず、短時間で簡易な作業により、容積増加を抑制しつつ、固液混合物の流動性を低下させることができる方法を提供する。【解決手段】本発明は、固液混合物と、前記固液混合物の流動性低下剤とを容器内で混合して低流動性混合物を得ることを含む、低流動性混合物の製造方法である。流動性低下剤は、繊維が絡み合った構造を有する粒状物を含み、粒状物は、平均粒子径が300μm以下かつBET法による比表面積が0.25m2/g以上100m2/g以下であり、又は(1−かさ密度/真密度)×100で計算される空隙率が50%以上かつBET法による比表面積が0.25m2/g以上100m2/g以下である。容器への低流動性混合物の搭載目標容積に対して、固液混合物が50容積%以上100容積%未満の量で混合され、かつ固液混合物及び流動性低下剤の使用容積の合計が容器への低流動性混合物の搭載目標容積を超える。【選択図】図1
MANUFACTURING METHOD OF LOW FLUID MIXTURE
低流動性混合物の製造方法
AIHARA KEIICHI (Autor:in) / FUJII SHIGEATSU (Autor:in) / MIYAMOTO MITSUYA (Autor:in) / OYA YOHEI (Autor:in) / TERAMURA TOSHIFUMI (Autor:in) / MINAGAWA HIDEAKI (Autor:in) / OYANE YUICHI (Autor:in)
15.06.2017
Patent
Elektronische Ressource
Japanisch
RECYCLED ASPHALT MIXTURE MANUFACTURING METHOD AND RECYCLED ASPHALT MIXTURE
Europäisches Patentamt | 2020