CEMENT CLINKER COMPOSITION AND PORTLAND CEMENT COMPOSITION
PROBLEM TO BE SOLVED: To provide a cement clinker composition that improves the strength development of concrete and mortar, and to provide a portland cement composition containing the cement clinker composition.SOLUTION: There is provided a cement clinker composition in which the proportion of 3CaO-SiOcalculated by the Bogue equation is 50 to 75 mass%, the proportion of 2CaO-SiOis 5 to 25 mass%, the proportion of the sum of 3CaO-AlOand 4CaO-AlO-FeOis 10 to 25 mass%, and MgO, SO, and F are contained and the content of MgO is 0.5 to 3.0 mass%, the content of SOis 0.3 to 1.5 mass%, the content of F is 100 to 800 mass ppm, and the content of MgO, SO, and F satisfies the relationship of the following formula (1). A portland cement composition comprising the cement clinker composition and gypsum. 1000≤(content of MgO(mass%))×(content of F (mass ppm)F)÷(content of SO(mass%))≤1800 (1).SELECTED DRAWING: None
【課題】コンクリートやモルタルの強度発現性を向上させるセメントクリンカ組成物およびそのセメントクリンカ組成物を含むポルトランドセメント組成物の提供。【解決手段】ボーグ式で算出された3CaO・SiO2の割合が50〜75質量%、2CaO・SiO2の割合が5〜25質量%、3CaO・Al2O3及び4CaO・Al2O3・FeO3の合計の割合が10〜25質量%、、MgO、SO3及びFを含み、MgOの含有量が0.5〜3.0質量%、SO3の含有量が0.3〜1.5質量%、Fの含有量が100〜800質量ppm、MgO、SO3およびFの含有量が下記の式(1)の関係を満たすセメントクリンカ組成物。このセメントクリンカ組成物、石膏とを含むポルトランドセメント組成物。1000≦(MgOの含有量(質量%))×(Fの含有量(質量ppm))÷(SO3の含有量(質量%))≦1800(1)【選択図】なし
CEMENT CLINKER COMPOSITION AND PORTLAND CEMENT COMPOSITION
PROBLEM TO BE SOLVED: To provide a cement clinker composition that improves the strength development of concrete and mortar, and to provide a portland cement composition containing the cement clinker composition.SOLUTION: There is provided a cement clinker composition in which the proportion of 3CaO-SiOcalculated by the Bogue equation is 50 to 75 mass%, the proportion of 2CaO-SiOis 5 to 25 mass%, the proportion of the sum of 3CaO-AlOand 4CaO-AlO-FeOis 10 to 25 mass%, and MgO, SO, and F are contained and the content of MgO is 0.5 to 3.0 mass%, the content of SOis 0.3 to 1.5 mass%, the content of F is 100 to 800 mass ppm, and the content of MgO, SO, and F satisfies the relationship of the following formula (1). A portland cement composition comprising the cement clinker composition and gypsum. 1000≤(content of MgO(mass%))×(content of F (mass ppm)F)÷(content of SO(mass%))≤1800 (1).SELECTED DRAWING: None
【課題】コンクリートやモルタルの強度発現性を向上させるセメントクリンカ組成物およびそのセメントクリンカ組成物を含むポルトランドセメント組成物の提供。【解決手段】ボーグ式で算出された3CaO・SiO2の割合が50〜75質量%、2CaO・SiO2の割合が5〜25質量%、3CaO・Al2O3及び4CaO・Al2O3・FeO3の合計の割合が10〜25質量%、、MgO、SO3及びFを含み、MgOの含有量が0.5〜3.0質量%、SO3の含有量が0.3〜1.5質量%、Fの含有量が100〜800質量ppm、MgO、SO3およびFの含有量が下記の式(1)の関係を満たすセメントクリンカ組成物。このセメントクリンカ組成物、石膏とを含むポルトランドセメント組成物。1000≦(MgOの含有量(質量%))×(Fの含有量(質量ppm))÷(SO3の含有量(質量%))≦1800(1)【選択図】なし
CEMENT CLINKER COMPOSITION AND PORTLAND CEMENT COMPOSITION
セメントクリンカ組成物およびポルトランドセメント組成物
YAMADA AKIRA (Autor:in) / MIYAWAKI KENJI (Autor:in)
28.09.2017
Patent
Elektronische Ressource
Japanisch
IPC:
C04B
Kalk
,
LIME
PORTLAND CEMENT CLINKER, CEMENT COMPOSITION AND METHOD FOR PRODUCING PORTLAND CEMENT CLINKER
Europäisches Patentamt | 2024
|PORTLAND CEMENT CLINKER, CEMENT COMPOSITION AND METHOD FOR PRODUCING PORTLAND CEMENT CLINKER
Europäisches Patentamt | 2023
|PORTLAND CEMENT CLINKER, CEMENT COMPOSITION, AND METHOD FOR PRODUCING PORTLAND CEMENT CLINKER
Europäisches Patentamt | 2023
|CEMENT CLINKER COMPOSITION AND PORTLAND CEMENT COMPOSITION
Europäisches Patentamt | 2019
|PORTLAND CEMENT CLINKER, CEMENT COMPOSITION, AND METHOD FOR PRODUCING PORTLAND CEMENT CLINKER
Europäisches Patentamt | 2025
|