Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
CERAMIC MATRIX COMPOSITE COMPONENT, GAS TURBINE SEAL ASSEMBLY, AND METHOD OF FORMING CERAMIC MATRIX COMPOSITE COMPONENT
PROBLEM TO BE SOLVED: To provide a high temperature seal with improved flexibility that better conforms to misaligned seal slots and realizes less leakage, better high temperature sealing, improved gas turbine performance, or combinations thereof.SOLUTION: A gas turbine seal assembly includes a gas turbine component and a gas turbine seal component contacting the gas turbine component so as to form a seal between the two components. The gas turbine seal component comprises multiple ceramic matrix composite plies 12 bonded together, and has: a bond-inhibiting coating 14 selectively arranged on a non-bonding portion of a first surface of the ceramic matrix composite plies 12; and a bonding portion 16 without the bond-inhibiting coating 14. The bonding portion 16 and a second surface of a neighboring ceramic matrix composite ply 12 form multi-ply bonding to each other. Thereby, a ceramic matrix composite component is formed.SELECTED DRAWING: Figure 1
【課題】柔軟性が改善された高温シールを提供し、アライメント不良のシール溝によりよく適合し、漏れが少ないよりよい高温シーリング並びに改善されたガスタービン性能、又はこれらの組合せの提供。【解決手段】ガスタービンシール組立品は、ガスタービン部品、及びガスタービン部品と接触しているガスタービンシール部品を含み、2つの部品間のシールを形成する。ガスタービンシール部品は、一緒に結合された多層のセラミックマトリックス複合材プライ12からなり、セラミックマトリックス複合材プライ12の第1の表面は非結合部分上に選択配置された結合阻害被覆14と、結合阻害被覆14のない結合部分16を有し、この結合部分16で、隣接するセラミックマトリックス複合材プライ12の第2の表面に相互に多層結合することによりセラミックマトリックス複合材部品を形成するガスタービン組立品。【選択図】図1
CERAMIC MATRIX COMPOSITE COMPONENT, GAS TURBINE SEAL ASSEMBLY, AND METHOD OF FORMING CERAMIC MATRIX COMPOSITE COMPONENT
PROBLEM TO BE SOLVED: To provide a high temperature seal with improved flexibility that better conforms to misaligned seal slots and realizes less leakage, better high temperature sealing, improved gas turbine performance, or combinations thereof.SOLUTION: A gas turbine seal assembly includes a gas turbine component and a gas turbine seal component contacting the gas turbine component so as to form a seal between the two components. The gas turbine seal component comprises multiple ceramic matrix composite plies 12 bonded together, and has: a bond-inhibiting coating 14 selectively arranged on a non-bonding portion of a first surface of the ceramic matrix composite plies 12; and a bonding portion 16 without the bond-inhibiting coating 14. The bonding portion 16 and a second surface of a neighboring ceramic matrix composite ply 12 form multi-ply bonding to each other. Thereby, a ceramic matrix composite component is formed.SELECTED DRAWING: Figure 1
【課題】柔軟性が改善された高温シールを提供し、アライメント不良のシール溝によりよく適合し、漏れが少ないよりよい高温シーリング並びに改善されたガスタービン性能、又はこれらの組合せの提供。【解決手段】ガスタービンシール組立品は、ガスタービン部品、及びガスタービン部品と接触しているガスタービンシール部品を含み、2つの部品間のシールを形成する。ガスタービンシール部品は、一緒に結合された多層のセラミックマトリックス複合材プライ12からなり、セラミックマトリックス複合材プライ12の第1の表面は非結合部分上に選択配置された結合阻害被覆14と、結合阻害被覆14のない結合部分16を有し、この結合部分16で、隣接するセラミックマトリックス複合材プライ12の第2の表面に相互に多層結合することによりセラミックマトリックス複合材部品を形成するガスタービン組立品。【選択図】図1
CERAMIC MATRIX COMPOSITE COMPONENT, GAS TURBINE SEAL ASSEMBLY, AND METHOD OF FORMING CERAMIC MATRIX COMPOSITE COMPONENT
セラミックマトリックス複合材部品、ガスタービンシール組立品、及びセラミックマトリックス複合材部品を形成する方法
HAFNER MATTHEW TROY (Autor:in) / ITZEL GARY MICHAEL (Autor:in) / JOHN MCCONNELL DELVAUX (Autor:in)
09.11.2017
Patent
Elektronische Ressource
Japanisch
Europäisches Patentamt | 2017
|Europäisches Patentamt | 2020
|CERAMIC MATRIX COMPOSITE COMPONENT AND METHOD OF PRODUCING CERAMIC MATRIX COMPOSITE COMPONENT
Europäisches Patentamt | 2021
|CERAMIC MATRIX COMPOSITE COMPONENT AND PROCESS OF PRODUCING CERAMIC MATRIX COMPOSITE COMPONENT
Europäisches Patentamt | 2017
|CERAMIC MATRIX COMPOSITE COMPONENT AND PROCESS OF PRODUCING CERAMIC MATRIX COMPOSITE COMPONENT
Europäisches Patentamt | 2017
|