REINFORCEMENT METHOD FOR CONCRETE COLUMN
PROBLEM TO BE SOLVED: To provide a reinforcement method for a concrete column, in which a good-quality earthquake strengthening mortar layer inhibiting the appearance of a crack can be easily formed with small thickness on an outer peripheral part of the existing concrete column.SOLUTION: In a reinforcement method, an earthquake strengthening mortar layer 10 with a small thickness of 40-70 mm, within which reinforcements 11 and 12 are arranged, is formed on an outer peripheral part of an existing concrete column 20 so as to apply earthquake strengthening. The reinforcement method includes: a bar arrangement step of arranging the reinforcements 11 and 12; a spraying method of spraying sprayed mortar 15; a finishing step of performing surface finish of the formed mortar layer 10; and a curing step of curing the mortar layer 10. In the spraying step, the sprayed mortar 15 with a slump value of 8-13 cm, a drying shrinkage rate of 0.06% or less, an adhesive strength of 0.1 N/mmor more and a compression strength of 50.0 N/mmor more is sprayed. The sprayed mortar 15 is separately sprayed on inside and outside layers 15a and 15b.SELECTED DRAWING: Figure 1
【課題】ひび割れの発生が抑制された品質の良好な耐震補強用のモルタル層を、薄い厚さで既存のコンクリート柱の外周部分に容易に形成できるようにするコンクリート柱の補強工法を提供する。【解決手段】既存のコンクリート柱20の外周部分に、内部に鉄筋11,12が配筋された40〜70mmの薄い厚さの耐震補強用のモルタル層10を形成して耐震補強する補強工法であって、鉄筋11,12を配筋する配筋工程と、吹付けモルタル15を吹き付ける吹付け工程と、形成されたモルタル層10の表面仕上げを行う仕上げ工程と、モルタル層10の養生を行う養生工程とを含んで構成される。吹付け工程では、スランプ値が8〜13cmであり、乾燥収縮率が0.06%以下、付着強度が0.1N/mm2以上、圧縮強度が50.0N/mm2以上である吹付けモルタル15を吹き付ける。吹付けモルタル15は、内側層15aと外側層15bとに分けて吹き付ける。【選択図】図1
REINFORCEMENT METHOD FOR CONCRETE COLUMN
PROBLEM TO BE SOLVED: To provide a reinforcement method for a concrete column, in which a good-quality earthquake strengthening mortar layer inhibiting the appearance of a crack can be easily formed with small thickness on an outer peripheral part of the existing concrete column.SOLUTION: In a reinforcement method, an earthquake strengthening mortar layer 10 with a small thickness of 40-70 mm, within which reinforcements 11 and 12 are arranged, is formed on an outer peripheral part of an existing concrete column 20 so as to apply earthquake strengthening. The reinforcement method includes: a bar arrangement step of arranging the reinforcements 11 and 12; a spraying method of spraying sprayed mortar 15; a finishing step of performing surface finish of the formed mortar layer 10; and a curing step of curing the mortar layer 10. In the spraying step, the sprayed mortar 15 with a slump value of 8-13 cm, a drying shrinkage rate of 0.06% or less, an adhesive strength of 0.1 N/mmor more and a compression strength of 50.0 N/mmor more is sprayed. The sprayed mortar 15 is separately sprayed on inside and outside layers 15a and 15b.SELECTED DRAWING: Figure 1
【課題】ひび割れの発生が抑制された品質の良好な耐震補強用のモルタル層を、薄い厚さで既存のコンクリート柱の外周部分に容易に形成できるようにするコンクリート柱の補強工法を提供する。【解決手段】既存のコンクリート柱20の外周部分に、内部に鉄筋11,12が配筋された40〜70mmの薄い厚さの耐震補強用のモルタル層10を形成して耐震補強する補強工法であって、鉄筋11,12を配筋する配筋工程と、吹付けモルタル15を吹き付ける吹付け工程と、形成されたモルタル層10の表面仕上げを行う仕上げ工程と、モルタル層10の養生を行う養生工程とを含んで構成される。吹付け工程では、スランプ値が8〜13cmであり、乾燥収縮率が0.06%以下、付着強度が0.1N/mm2以上、圧縮強度が50.0N/mm2以上である吹付けモルタル15を吹き付ける。吹付けモルタル15は、内側層15aと外側層15bとに分けて吹き付ける。【選択図】図1
REINFORCEMENT METHOD FOR CONCRETE COLUMN
コンクリート柱の補強工法
HIRONAKA TETSUYA (Autor:in) / YAMAGUCHI OSAMU (Autor:in) / MISAWA TAKASHI (Autor:in)
11.10.2018
Patent
Elektronische Ressource
Japanisch
REINFORCEMENT METHOD OF CONCRETE COLUMN, AND CONCRETE COLUMN
Europäisches Patentamt | 2021
|REINFORCED CONCRETE COLUMN SEISMIC REINFORCEMENT DEVICE
Europäisches Patentamt | 2020
|